Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE 2028-1

Main features

  • Transparent UV-Stable Bonding
  • 6 to 8-Minute Pot Life
  • 60% Cured Elongation

Product Description

ARALDITE® 2028-1 is a two-component, cold-curing polyurethane structural adhesive that mixes 1:1 by weight or volume to form a transparent adhesive. It is UV stable and suitable for bonding a variety of metal and plastic substrates, with additional published test data for composites, glass and wood. The system provides a 6–8 minute pot life in a static mixer and about 6 minutes for a 100 g mix at 25°C, supporting fast assembly. A thin 0.05–0.10 mm adhesive layer is recommended for greatest lap shear under the stated test approach. The mixed adhesive has specified lap shear strength above 8 MPa at 23°C, while typical cured-property data include 6.6 N/mm roller peel, 60% elongation at break and environmental-aging evaluations.

Key features

  • Transparent, UV-stable formulation: Forms a transparent mixed adhesive for assemblies where bondline appearance and light exposure are selection factors.
  • Fast 1:1 processing: Mixes equally by weight or volume and provides a 6–8 minute pot life in a static mixer.
  • Multi-substrate structural bonding: Suitable for selected metal and plastic substrates, with specified mixed-adhesive lap shear strength above 8 MPa at 23°C.

Applications / Suitable for

  • Selected metal bonding, including aluminium, steels, copper and brass
  • Selected plastics and composites, including GRP, CFRP, SMC, ABS, PVC, PMMA, polycarbonate and polyamides
  • Glass and wood bonding evaluated under the stated cure conditions
Product Family

ARALDITE 2028-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life Pot Life
7 minutes
Specific Gravity Specific Gravity
1.12
Physical Properties
Viscosity (Part A) Viscosity (Part A)
3000 mPa.s
Viscosity (Part B) Viscosity (Part B)
9000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Values distinguish Component A, Component B and the mixed adhesive where applicable. Specified and typical values retain their stated source status and conditions.

Property Value Unit Method / condition
Colour Transparent / translucent / transparent — Component A / Component B / mixed adhesive; visual method A112; specified
Specific gravity 1.12 / 1.12 / 1.12 — Component A / Component B / mixed adhesive
Viscosity at 25°C 3–4.5 / 7–11 Pa·s Component A / Component B; method A191; specified
Mix ratio by weight 100:100 parts Component A : Component B
Mix ratio by volume 100:100 parts Component A : Component B
Pot life in static mixer 6–8 min Mixed adhesive
Pot life About 6 min 100 g mixed mass at 25°C
Flashpoint >100 °C Adhesive system
Technical properties

After-processing / final-state properties

Except for the specified mixed-adhesive lap shear value, the values below are typical laboratory data and are not guaranteed design values.

Property Value Unit Method / condition
Lap shear strength at 23°C >8 MPa Mixed adhesive; method A501; specified
Roller peel 6.6 N/mm Typical average; ISO 4578; cure 16 h at 40°C
Glass transition temperature 13 °C Typical average; DMA; cure 16 h at 40°C
Tensile strength at 23°C 11 MPa Typical average; ISO 527
Tensile modulus 16 MPa Typical average; ISO 527
Elongation at break 60 % Typical average; ISO 527
Lap shear on wood / glass 7 / 7 MPa Typical average; cure 16 h at 40°C
Lap shear after thermal cycling 12.8 MPa Typical average; 100 cycles of 6 h from −30°C to 70°C