ARALDITE AV 8503
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- One-Minute Fixturing Time
- Heat-Resistant Bonding Service
- 1:1 Controlled Mixing
Product Description
ARALDITE® AV 8503 Resin / Hardener HV 8503 is a two-component epoxy adhesive paste developed for bonding sheet molding compound, plastics, and metals. The blue resin and beige hardener mix at a convenient 1:1 ratio by volume and form a non-sag paste with approximately 100 minutes of pot life at 25°C. The adhesive combines good flexibility with heat resistance and can achieve rapid handling strength using a heated fixture. Its surface-preparation requirements are limited to a dry wipe before bonding, supporting straightforward assembly processes where controlled paste application and accelerated heat cure are required.
Key features
- Rapid heat fixture: Reaches fixture strength in approximately one minute on a fixture heated to 116°C.
- Flexible cured epoxy: Provides 15% elongation with a Shore D hardness of 78.
- Convenient paste mixing: Uses a 1:1 mix ratio by volume with good weldability and non-sag application behavior.
Applications / Suitable for
- Sheet molding compound bonding
- Plastic assembly
- Metal bonding