ARALDITE CY179-1
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Configurable Heat-Cure Formulation
- Electrical Casting Resin Component
- Encapsulation System Processing Base
Product Description
ARALDITE CY 179-1 Epoxy Resin is a cycloaliphatic epoxy resin component for heat-curing casting and encapsulation systems. The resin is selected as the epoxy component in formulations where the hardener and accelerator are chosen separately for the required process and cured-property profile. It is used in electrical and electronic casting or encapsulation systems, with processing and final performance determined by the complete formulation and cure schedule. CY 179-0.625remains a component-level product rather than a ready-to-use casting compound, so mixed-system properties apply only to the specified resin, hardener, accelerator, ratio, and cure conditions.
Key features
- Cycloaliphatic epoxy component: CY 179-1 serves as the resin base in specified casting and encapsulation formulations.
- Configurable heat-cure processing: Hardener and accelerator selection defines the complete system and cure profile.
- Electrical casting system role: The resin is used in electrical and electronic casting or encapsulation systems.
Applications
Electrical and electronic casting or encapsulation within specified CY 179-1 resin systems.