AXAREL 1000
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- MIL-PRF-680 Type I Approved Cleaner
- 60 ppm Nonvolatile Residue
- Multi-Soil Manual/Immersion Cleaning
Product Description
AXAREL™ 1000 Solvent Cleaner is an approved MIL-PRF-680 Type I cleaner for precision cleaning and degreasing. It is suitable for replacing isopropyl alcohol, acetone, methyl ethyl ketone, mineral spirits, P-D-680 solvents, and other low-flash-point flammable solvents in supported applications. The cleaner is designed for hand wiping, immersion cleaning, and airless vacuum hydrocarbon equipment, removing greases, mineral and synthetic oils, coolants, rust inhibitors, fingerprint oils, dust, and particulate matter while leaving very low surface residues. AXAREL™ 1000 is compatible with many polymeric substrates and elastomers and is safe for use with ferrous and non-ferrous alloys.
Key features
- MIL-PRF-680 Type I approved solvent cleaner.
- Low vapor pressure of 0.78 mmHg at 20°C.
- Low surface residue with 60 ppm non-volatile residue.
- Good solvency for oils, greases, coolants, rust inhibitors, and particulate soils.
- Multiple process options including manual wiping, immersion, and airless vacuum cleaning.
- Broad material compatibility with many polymers, elastomers, and ferrous and non-ferrous alloys.
Applications / Suitable for
- Manual cleaning and degreasing by brush, pad, or cloth.
- Immersion cleaning at full concentration.
- Airless vacuum hydrocarbon cleaning systems.
Technical Specifications
Thermal Properties
General Properties
Additional Information
AXAREL™ 1000 Solvent Cleaner
A precision cleaning and degreasing solvent for manual wiping, immersion cleaning, and airless vacuum hydrocarbon equipment. AXAREL™ 625removes a broad range of hydrocarbon and particulate soils while leaving very low surface residues.

As-supplied properties
Typical property data are provided for product evaluation and are not specification limits.
| Property | Typical value | Condition / context |
|---|---|---|
| Odor | Essentially odorless | As supplied |
| Flash point | 53°C (127°F) | As reported |
| Specific gravity | 0.76 | At 25°C |
| Viscosity | 1.36 cP | At 25°C |
| Distillation range | 179–187°C (354–369°F) | As reported |
| Vapor pressure | 0.78 mmHg | At 20°C |
| Kauri-butanol value | 29 | As reported |
| Evaporation rate | 0.1 | n-butyl acetate = 1 |
| Surface tension | 24.1 dynes/cm | At 25°C |
| Non-volatile residue | 60 ppm | As reported |
Cleaning process
AXAREL™ 1000 is used at full concentration. Select the cleaning method based on the part geometry, soil load, substrate, process equipment, and required cleanliness.
Soils removed
Approvals and testing
The supplied technical data sheet lists the following product-specific approvals, qualifications, and test references. Users should confirm current revision, scope, site, and application requirements before specification.
| Organization / standard | Listed scope |
|---|---|
| MIL-PRF-680 | Type I Degreasing Solvent, QPL, DS-0020 |
| Airbus | A330 Maintenance Manual Item 11-002 Dry Cleaning Solvent; Consumable Materials List reference |
| Boeing | BAC 5750 Solvent Cleaning, optional to P-D-680 specification, PSD 6-88 |
| Honeywell Aerospace | Per MIL-PRF-680 qualifications |
| Lockheed Martin | STP57-201, Revision H |
| Pratt & Whitney | PMC 9045, POP 350 cleaning/degreasing of metallic engine hardware |
| Rolls-Royce | CSS276 and OMat 102 |
| United Airlines | SOL3001-1 |
| ASTM testing | F1110, F483, F945, D130, D1296, and D1353 |
Environmental and regulatory information
| Attribute | Reported status / value |
|---|---|
| Ozone depletion potential | Zero |
| Global warming potential | Low |
| Hazardous air pollutant | No |
| VOC | 760 g/L |
| SARA | Not regulated |
| NESHAPs | Not regulated |
| RCRA | Regulated |
Available in 31 lb (14 kg) pails and 348 lb (158 kg) drums. Shelf life is 36 months when stored in the original sealed container above 10°C (50°F). Listed NSNs include 6850-01-474-2302, 6850-01-474-2309, 6850-01-474-2313, and 6850-01-163-1888. Consult the current Safety Data Sheet for handling and disposal requirements.