BIOACT 105
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- High-Solvency Aerospace Soil Removal
- Manual-Wipe or Immersion Cleaning
- AMS 3167 Aerospace Conformance
Product Description
BIOACT 105 is a high-purity, fast-drying solvent cleaner for manual degreasing, damp-dry surface preparation, and room-temperature immersion cleaning. Its citrus-terpene, alcohol, and hydrocarbon blend combines a Kauri-Butanol value above 150 with low surface residue and a vapor pressure of 1.5 mmHg at 20°C. The cleaner removes adhesives, greases, corrosion inhibitors, paint overspray, silicones, waxes, and other industrial soils. It is compatible with many polymeric substrates and elastomers and can be used on ferrous and non-ferrous alloys. BIOACT 105 also conforms to AMS 3167 and is documented for multiple aerospace OEM cleaning processes.
Key features
- High solvency: Kauri-Butanol value greater than 150.
- Fast-drying, low-residue cleaning: Supports controlled manual and immersion cleaning.
- Flexible application: Suitable for hand wiping, damp-dry surface preparation, and room-temperature immersion.
- Broad soil-removal scope: Removes adhesives, greases, corrosion inhibitors, paint overspray, silicones, waxes, and other documented soils.
- Material compatibility: Documented for many polymeric substrates and elastomers and for ferrous and non-ferrous alloys.
- Aerospace process acceptance: Conforms to AMS 3167 and is documented for multiple aerospace OEM cleaning processes.
Applications / Suitable for
- Manual cleaning and degreasing
- Surface preparation before bonding, sealing, coating, or painting
- Room-temperature immersion and soak-tank cleaning
- Commercial and general aviation maintenance and precision cleaning
Technical Specifications
No specifications available.
Additional Information
BIOACT 105
BIOACT 105 is a high-purity, fast-drying solvent cleaner for manual degreasing, damp-dry surface preparation, and room-temperature immersion cleaning. Its Kauri-Butanol value above 150 supports removal of difficult industrial soils, while low surface residue and compatibility with many alloys, polymers, and elastomers support controlled cleaning across aerospace and precision-manufacturing workflows.

As-Supplied Properties
Typical product data for evaluation. These values are not guaranteed specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Clear liquid | — | As supplied |
| Odor | Mild citrus/alcohol | — | As supplied |
| Flash point | 41 (105) | °C (°F) | Closed cup |
| Specific gravity | 0.80 | — | 25°C |
| Viscosity | 1.6 | cP | 25°C |
| Vapor pressure | 1.5 | mmHg | 20°C |
| Kauri-Butanol value | >150 | — | Typical solvency value |
Application and Processing
Choose the cleaning method based on the substrate, soil, and downstream process. Confirm compatibility under actual use conditions before broad implementation.
Application Sequence
Store BIOACT 105 in its original, sealed container above 50°F (10°C). The documented shelf life is 36 months under these conditions. Keep the container tightly closed in a cool, well-ventilated storage area and consult the current SDS for complete safe-handling, fire-prevention, and disposal requirements.
Technical Guidance
Approvals and Conformance
| Issue or observation | Source-supported guidance | Qualification boundary |
|---|---|---|
| Aerospace general | Conforms to AMS 3167. | Confirm the current specification revision and customer or program requirements before use. |
| Boeing and Douglas | Boeing D6-17487 Rev L, except ASTM F-484; BSS 7432; Douglas CSD #1. | Apply only within the stated tests, exclusions, and process scope. |
| OEM process listings | Bell Helicopter Bulletin 1915; Bombardier BAPS 180-009 General; CFM CP# 2719 Rev 76; GE Method 23 / C04-251 and listed alternatives; Gulfstream GAS115H; Honeywell C5049. | Use the exact OEM document, part, substrate, and cleaning method required by the program. |
| Engine manufacturer requirements | Pratt & Whitney SPOP 208, POP 1800-U, PMC 8929, and PWA 36604 Hot Corrosion; Rolls-Royce CSS No. 255 Type A and OMat 1/257S. | Do not extend acceptance beyond the named process or material scope. |
| Airline use | United Airlines SOL3001-17 and SOL3001-17WL10X12. | Verify the correct product form and current airline process document. |
| ASTM testing | ASTM F-945, F-1110, F-502, F-519, F-485, F-482, and F-2111. | Test completion does not create universal substrate or process suitability. |
Applications
BIOACT 105 supports full-strength manual and immersion cleaning where strong solvency, low surface residue, and controlled application are required.