BIOACT EC-7M
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- USDA-Certified Cleaning Product
- Solder-Flux, Paste, Oil, and Grease Removal
- Reduced Solvent Loss
Product Description
BIOACT™ EC-7M Solvent Cleaner & Defluxer is a USDA Certified Biobased, terpene-based electronics cleaner designed for manual wiping and immersion defluxing. The clear, low-viscosity liquid provides strong solvency for removing solder-flux residues, pastes, inks, oils, grease, and selected adhesive or coating residues from electronic and mechanical assemblies. Its low volatility helps reduce solvent loss during room-temperature cleaning processes.
Key features
- High-performance electronics cleaning: Designed to remove solder-flux residues and other organic contamination from electronic assemblies.
- Biobased terpene formulation: Uses high-purity, low-odor terpene solvents and is identified as a USDA Certified Biobased Product.
- Low-viscosity processing: Supplied at 0.8 cP at 25°C for manual wiping and immersion cleaning.
- Low volatility: Relatively slow evaporation helps limit solvent consumption during cleaning.
Applications / Suitable for
- Manual wiping of electronic and mechanical assemblies
- Room-temperature immersion defluxing
- Removal of solder fluxes, pastes, inks, oils, and grease
- Cleaning printed circuit boards, components, connectors, cables, and mechanical assemblies
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
Physical Properties
General Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied properties. Values are not intended for use as specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Terpene-based solvent cleaner and defluxer | — | As supplied |
| Appearance | Clear, free-flowing liquid | — | As supplied |
| Odor | Slight orange | — | As supplied |
| Boiling point | 169 (340) | °C (°F) | Typical value |
| Flash point | 47 (117) | °C (°F) | Tag closed cup |
| Specific gravity | 0.84 | — | At 25°C |
| Viscosity | 0.8 | cP | At 25°C |
| Kauri-butanol value | 67 | — | Cleaning-strength indicator |
| Surface tension | 33 | dynes/cm | Typical value |