VANTAGE BIOACT SC-10 ELECTRONICS CLEANER
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Fast-Drying Electronics Cleaner
- Multi-Soil Electronics Residue Removal
- Manual-Wipe or Immersion Cleaning
Product Description
VANTAGE BIOACT™ SC-10 Solvent Cleaner & Defluxer is a high-performance electronics cleaning solvent designed for manual wipe and immersion cleaning applications. Formulated with citrus terpenes and highly refined polar and non-polar solvents, it provides fast drying, excellent solvency, and low surface residue. BIOACT™ SC-10 is used to remove flux residues, uncured SMD adhesives, acrylic conformal coatings, tape residues, oils, greases, and other manufacturing contaminants from electronic assemblies while serving as an alternative to isopropyl alcohol (IPA) and hydrocarbon cleaners. :contentReference[oaicite:0]{index=0}
Key Features
- Fast-drying solvent cleaner with excellent solvency and low surface residue.
- Removes multiple electronic contaminants, including flux residues, uncured SMD adhesives, acrylic conformal coatings, and tape residues.
- IPA replacement suitable for manual wipe and immersion cleaning applications.
Applications / Suitable for
- Cleaning printed circuit board assemblies (PCBAs)
- Manual electronic assembly cleaning
- Immersion cleaning of electronic assemblies
- Removal of flux residues and ionic contamination
- Removal of uncured SMD adhesives, acrylic conformal coatings, tape residues, oils, greases, and marking inks
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
General Properties
Physical Properties
Electrical Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Appearance | Liquid | — | As supplied |
| Odor | Mild | — | Published property |
| Flash Point | 41 | °C | 105 °F |
| Specific Gravity (25°C) | 0.80 | — | 25°C |
| Viscosity (25°C) | 1.6 | cP | 25°C |
| Vapor Pressure (20°C) | 1.5 | mm Hg | 20°C |
| Kauri-Butanol (KB) Value | >150 | — | Published property |
| Dielectric Strength | 40.1 | kV | Published property |