BIOACT SC-22
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Rinse-Free Immersion or Ultrasonic Cleaning
- 62 deg C Flash Point
- 0.5 mmHg Vapor Pressure
Product Description
BIOACT™ SC-22 Solvent Cleaner & Defluxer is a rinse-free solvent cleaner formulated from a proprietary mixture of modified alcohols. Designed for ambient or heated immersion cleaning, it removes uncured surface-mount adhesives and raw solder pastes from stencils and misprinted circuit assemblies. It also removes rosin, no-clean, and water-soluble flux residues from circuit assemblies and can be used as an alternative to isopropyl alcohol in supported cleaning processes.
Key features
- Rinse-free cleaning: Supports solvent cleaning without a subsequent water-rinse stage.
- Broad residue removal: Removes uncured SMD adhesives, raw solder pastes, and rosin, no-clean, and water-soluble flux residues.
- Ambient or heated processing: Suitable for use from 70 to 125°F (20 to 49°C).
- High flash point: Provides a flash point of 144°F (62°C), Pensky-Martens closed cup.
Applications / Suitable for
- Ambient or heated immersion cleaning
- Ultrasonic cleaning processes
- Cleaning stencils and misprinted circuit assemblies
- Removal of uncured SMD adhesives, raw solder pastes, and flux residues
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied and recommended process properties. Values are not intended for use as specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Rinse-free solvent cleaner and defluxer | — | Proprietary mixture of modified alcohols |
| Appearance | Colorless to yellow liquid | — | As supplied |
| Flash point | 144 (62) | °F (°C) | Pensky-Martens closed cup |
| Specific gravity | 0.88 ± 0.01 | — | At 25°C |
| Viscosity | 3 | cPs | At 25°C |
| Vapor pressure | 0.5 | mmHg | At 20°C |
| Kauri-butanol value | >150 | — | Typical value |
| Use concentration | 100 | % | Immersion or ultrasonic cleaning |
| Recommended operating temperature | 70–125 (20–49) | °F (°C) | Immersion or ultrasonic cleaning |
| Ozone depletion potential | 0 | — | Reported in the supplied TDS |