BONDERITE C-AK LS
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Rolling-Oil Steel-Strip Cleaning
- Dip, Spray, or Electrolytic Cleaning
- Oil-Separating Emulsion Behavior
Product Description
BONDERITE® C-AK 71110 (LS-TP1 (DE)) is a pale-yellow, clear, highly alkaline, heavy-duty industrial cleaner for steel-strip processing. Suitable for dip, spray, and electrolytic cleaning, it supports rapid removal of rolling oils before continuous annealing, electroplating, and galvanizing. Its surfactant blend promotes penetration and emulsification across a range of rolling oils, while the resulting emulsions are formulated to separate on standing for subsequent oil removal and effluent treatment.
Key features
- Heavy-duty steel-strip cleaning: Formulated for fast, efficient removal of rolling oils before continuous annealing, electroplating, and galvanizing.
- Flexible process application: Suitable for dip, spray, and electrolytic cleaning systems.
- Oil-separating emulsion behavior: Allows emulsified oil to separate on standing for subsequent removal and effluent processing.
Applications / Suitable for
- Cleaning steel strip before continuous annealing
- Cleaning steel strip before electroplating
- Cleaning steel strip before galvanizing
- Dip-cleaning systems
- Spray-cleaning systems
- Electro-cleaning systems
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Supplier-published as-supplied characteristics and storage information for BONDERITE® C-AK 71110.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Alkaline industrial cleaner | — | Heavy-duty liquid cleaner for steel strip |
| Appearance | Pale yellow, clear liquid | — | As supplied |
| Specific gravity | 1.33 | — | At 20°C |
| Storage-temperature range | 0 to 40 | °C | Supplier-published storage condition |
| Shelf life | 24 | months | In unopened original packaging |