BONDERITE M-CR 1201
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- MIL-DTL-81706 Brush-Application Approval
- Ready-to-Use Without Titration or Adjustment
- Integral Gold-to-Tan Aluminum Coating
Product Description
BONDERITE M-CR 1201 AERO is a nonflammable, chromic acid-based liquid chromate conversion coating used for corrosion protection and paint adhesion on aluminum surfaces. It is approved to MIL-DTL-81706 for brush application and is used as received for MIL-DTL-5541 work, without adjustment or titration. The coating formed is gold to tan in color and becomes part of the aluminum surface. Availability of this product has been affected by REACH-related regulatory restriction in the UK and European markets.
Key features
- MIL-DTL-81706 Brush-Application Approval: approved for brush application under MIL-DTL-81706
- Ready-to-Use, No Titration Required: used as received for MIL-DTL-5541 work without adjustment or titration
- Integral Gold-to-Tan Aluminum Coating: forms a gold-to-tan chromate coating that becomes part of the aluminum surface
Applications
Brush or wipe application of chromate conversion coating to aluminum surfaces.