BONDERITE M-FE 101

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE M-FE 101

Main features

  • One-Step Steel Cleaning and Phosphating
  • Improved Paint Adhesion, Coating Durability, and Corrosion Resistance
  • Steam Gun and High-Pressure Manual Applications

Product Description

BONDERITE® M-FE 101 is a concentrated iron phosphate metal pretreatment designed to simultaneously clean steel surfaces and form a corrosion-resistant, non-metallic amorphous phosphate conversion coating. Developed for steam gun and high-pressure manual applications, it improves paint adhesion, enhances coating durability, and extends the service life of painted components used in metal fabrication and maintenance operations. :contentReference[oaicite:0]{index=0}

Key Features

  • Iron phosphate conversion coating for steel surface pretreatment.
  • Simultaneously cleans and phosphates steel surfaces.
  • Improves paint adhesion and coating durability.
  • Provides corrosion-resistant amorphous phosphate coating.
  • Suitable for steam gun and high-pressure manual application.

Applications / Suitable for

  • Steel surface pretreatment
  • Paint preparation
  • Metal fabrication
  • Equipment maintenance
  • Steam gun application
  • High-pressure manual application
Product Family

BONDERITE M-FE 101

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

General Properties
Product Type Product Type
Iron phosphate conversion coating
Thermal Properties
Operating Temperature Operating Temperature
Typically 49–60°C (120–140°F) °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal pretreatment — Supplier classification
Product type Concentrated liquid — Supplier description
Primary chemistry Iron phosphate — Supplier specification
Application methods Steam gun, high-pressure manual application — Supplier recommendation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Total acid 2.0–6.0 points Operating range
Operating temperature 49–88 °C 120–190°F
Treatment time 1–10 minutes Supplier recommendation
Conversion coating Non-metallic amorphous iron phosphate — On treated steel
Performance Improves paint adhesion and corrosion resistance — Finished surface