BONDERITE M-FE HMF-1080

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE M-FE HMF-1080

Main features

  • Heavy-Metal-Free Multi-Metal Clean/Phosphate Process
  • Improved Paint Adhesion and Corrosion Resistance
  • Multi-Metal Spray-Tunnel Pretreatment

Product Description

BONDERITE® M-FE HMF-1080 is a heavy metal-free liquid iron phosphate pretreatment that simultaneously cleans and forms an amorphous iron phosphate conversion coating on steel, zinc-coated steels, and aluminum. Designed primarily for spray application in treatment tunnels, it provides excellent surface preparation prior to painting while improving corrosion resistance and paint adhesion across mixed-metal production lines.

Key Features

  • Simultaneously degreases and phosphates metal surfaces in a single process.
  • Heavy metal-free (HMF) formulation suitable for multi-metal treatment.
  • Produces a dense, adherent amorphous iron phosphate coating for improved paint adhesion.
  • Suitable for steel, galvanized steel, electrogalvanized steel, and aluminum.
  • Designed primarily for spray application in industrial pretreatment tunnels.

Applications / Suitable for

  • Steel
  • Electrogalvanized steel
  • Galvanized steel
  • Aluminum
  • Multi-metal pretreatment lines
  • Pre-paint surface preparation
  • Industrial spray pretreatment tunnels
Product Family

BONDERITE M-FE HMF-1080

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product Type Product Type
Iron phosphate pretreatment

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Iron phosphate metal pretreatment — Supplier classification
Product type Complete liquid cleaner / phosphating product — Supplier description
Appearance Clear liquid — As supplied
Color Colorless to pale yellow — As supplied
Density 1.12 g/cm³ Supplier value
10 g/L solution pH Approximately 3.5 — 10 g/L solution
Water solubility Readily miscible — Supplier description
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Working concentration 15–30 mL/L Recommended operating range
Operating temperature 45–65 °C Spray process
Contact time 90–180 seconds Recommended operating range
Spray pressure 1.5–2.5 bar Recommended operating range
Working bath pH 4.5–5.8 — Recommended operating range
Total acidity 3–6 points Recommended operating range
Conversion coating Dense amorphous iron phosphate film — Blue to iridescent, sometimes gray
Coating weight 0.3–0.8 g/m² Typical deposited coating