BONDERITE M-MN LUBRITE 2

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

BONDERITE M-MN LUBRITE 2

Main features

  • Oil-Absorptive Phosphate Lubricating Coating
  • Rapid Break-In and Reduced Scuffing
  • Corrosion-Resistant Oil-Finishing Surface

Product Description

BONDERITE® M-MN LUBRITE 2 is a manganese phosphate conversion coating formulated to produce nonmetallic, oil-absorptive coatings on iron and steel bearing surfaces. The resulting iron and manganese phosphate coating improves lubrication, reduces wear during component break-in, enhances corrosion resistance, and provides an excellent surface for oil finishing on precision mechanical components such as pistons, piston rings, liners, camshafts, tappets, and engine blocks.

Key Features

  • Produces oil-absorptive iron and manganese phosphate coatings for improved lubrication.
  • Reduces wear during component break-in by minimizing metal-to-metal contact.
  • Retards corrosion while providing an excellent surface for oil finishing.
  • Helps remove light machining scratches during the phosphating process.
  • Designed for precision iron and steel bearing surfaces.

Applications / Suitable for

  • Pistons
  • Piston rings
  • Cylinder liners
  • Camshafts
  • Tappets
  • Motor blocks
  • Iron and steel bearing surfaces
Product Family

BONDERITE M-MN LUBRITE 2

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product Type Product Type
Manganese phosphate conversion coating
Thermal Properties
Operating Temperature Operating Temperature
Typically 88–99°C (190–210°F) °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Manganese phosphate conversion coating — Supplier classification
Product type Phosphating chemical — Supplier description
Primary substrate Iron and steel bearing surfaces — Supplier recommendation
Bath make-up 120 lb (11 gal) per 100 gal working solution — Initial bath preparation
Bath aging Requires bath aging before production — Additive or steel wool treatment
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Operating temperature 205–210 °F Recommended operating range
Treatment time Approximately 15 minutes Immersion process
Total acid 11.5–12.5 points Operating control
Free acid 2.0–2.2 points Operating control
Iron (II) 0.2–0.3 % Bath control
Coating composition Iron and manganese phosphates — Finished coating
Performance Oil-absorptive, wear reducing, corrosion resistant — Finished coating