BOSTIK L7132K
Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission
Main features
- Two-Part High-Green-Strength Laminating
- Heat- and Creep-Resistant Bonding
- BMS 5-127G Aerospace Qualification
Product Description
Bostik L7132K is a two-part solvent-based thermoset adhesive kit consisting of L7132R adhesive and Boscodur® 24T crosslinker. It is specifically formulated for vacuum and pressure bonding of PVC films to wood, fiberboard, and other porous substrates. The system provides excellent green strength for immediate edge trimming after vacuum forming and develops tough, heat- and creep-resistant bonds with excellent adhesion to vinyl, particle board, polyolefin foams, plastics, and other laminating materials. The product meets BMS 5-127G Type III Class 2 & 3 product specification requirements for aerospace applications. :contentReference[oaicite:0]{index=0}
Key Features
- Two-part thermoset adhesive system designed for vacuum and pressure laminating applications.
- Excellent green strength allows immediate edge trimming after vacuum forming.
- Heat- and creep-resistant bonds using the Boscodur® 24T crosslinking system.
- Meets BMS 5-127G Type III Class 2 & 3 product specification for aerospace applications.
Applications / Suitable For
- Vacuum-form bonding of PVC films
- Aerospace interior decorative laminates
- Automotive door panels, dashboards, consoles and interior trim
- Decorative furniture laminates
- PVC-coated luggage shell construction
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | L7132R (Part A) | Boscodur® 24T (Part B) | Method / Condition |
|---|---|---|---|
| Appearance | Opaque liquid | Dark brown liquid | Typical physical property |
| Base | Linear saturated polyester | Polyisocyanate | Supplier classification |
| Solvent system | MEK blend | MEK | Supplier description |
| Total solids | 25.5% | 68% | Typical value |
| Density @ 25°C | 7.67 lb/gal (0.919 g/cm³) | 8.76 lb/gal (1.05 g/cm³) | Typical value |
| Viscosity | 100 cP | Thin liquid | Brookfield |
| Flash point (SCC) | 14°F (-10°C) | 29°F (-2°C) | Typical value |
| Mix ratio | 16 parts L7132R : 1 part Boscodur® 24T (by volume) | Supplier recommendation | |
| Shelf life | 9 months | 55–80°F (15–27°C), unopened containers | |
After-Processing / Final-State Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Wet adhesive application | 100–150 | g/m² | Applied to least porous laminating surface |
| Lamination temperature | 110–212 (41–100) | °F (°C) | Pressure lamination |
| Minimum cure temperature | 190 (88) | °F (°C) | Minimum 4 minutes |
| Vacuum pressure | Minimum 15 in Hg (51 kPa), 20 in Hg (68 kPa) preferred | — | Vacuum-form process |
| Pot life | 8 | hours | After mixing |
| Performance | Tough, heat- and creep-resistant bond with immediate edge trimming capability | — | Supplier description |