BOSTIK L7132R
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Two-Component High-Green-Strength Laminating
- Heat- and Creep-Resistant Bonding
- Wide Vacuum-Form Processing Window
Product Description
Bostik 7132R / Boscodur® 4 is a two-component adhesive system developed for vacuum-form bonding of PVC films to wood, fiberboard, and other porous substrates. The system combines Bostik 7132R with Boscodur® 4 crosslinker to produce strong, heat- and creep-resistant bonds while providing excellent green strength for immediate edge trimming after removal from the vacuum former. The adhesive also exhibits excellent adhesion to polyolefin foams, polyester films, laminating films, foils, sheet metal, and cellulosic materials, making it suitable for demanding transportation, furniture, and industrial laminating applications. :contentReference[oaicite:0]{index=0}
Key Features
- Two-component adhesive system designed for vacuum-form laminating of PVC films.
- Excellent green strength enables immediate edge trimming after vacuum forming.
- Heat- and creep-resistant bond achieved through the Boscodur® 4 crosslinking system.
- Wide processing window with excellent adhesion to vinyl, particle board, polyolefin foams, plastics, and cellulosic substrates.
Applications / Suitable For
- Vacuum-form bonding of PVC films
- Furniture decorative laminates
- Automotive interior trim, door panels, dashboards and consoles
- Aeronautic cabin interior laminates
- Luggage shell construction
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | 7132R (Part A) | Boscodur® 4 (Part B) | Method / Condition |
|---|---|---|---|
| Appearance | Amber liquid | Brown liquid | Typical physical property |
| Base | Linear saturated polyester | Polyisocyanate | Supplier classification |
| Total solids | 25.5% | 68% | Typical value |
| Viscosity | 100 cP | Thin liquid | Brookfield LVF #1, 60 rpm, 25°C |
| Density | 7.67 lb/gal | 8.76 lb/gal | Typical value |
| Flash point (SCC) | 14°F (-10°C) | 29°F (-2°C) | Typical value |
| Solvent system | MEK blend | MEK | Supplier description |
| Mix ratio | 20–24 parts 7132R : 1 part Boscodur® 4 (by volume) | Supplier recommendation | |
| Shelf life | 6 months at 55–80°F (15–27°C) | Storage recommendation | |
After-Processing / Final-State Properties
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Drying condition | 80°C for 1–3 minutes | — | Circulating air oven |
| Vacuum lamination temperature | 110–210°F (43–99°C) | — | Approximately 20 seconds or longer |
| Open pot life | 8 hours | — | After mixing |
| Handling strength | Immediate edge trimming after vacuum forming | — | Supplier description |
| Full cure | Up to 72 hours to 1 week | — | Application dependent |
| Performance | Heat- and creep-resistant bond with excellent edge-folding capability | — | Supplier description |