CONAP DS-1832
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Black Epoxy/Polyurethane Color Concentrate
- 18% Heat-Stable Black Pigment
- Filled/Unfilled Resin Addition Ranges
Product Description
CONAP® DS-1832 Black Color Concentrate is a black pigment concentrate for modifying epoxy and polyurethane resin systems used in electrical potting, casting, and encapsulation. The one-part concentrate contains heat-stable pigments and is documented for compatibility with most epoxy and urethane systems, with improved heat and light resistance. For unfilled systems, the published starting range is three to five parts concentrate per 100 parts base resin or curative, or two to four percent of the total mixed system. DS-1832 contains 18% black pigment and requires thorough mixing before use.
Key features
- Black resin-system concentrate: The product is formulated for epoxy and polyurethane potting, casting, and encapsulation systems.
- Heat-stable pigment: The concentrate is documented for improved heat and light resistance.
- Controlled addition range: Published use levels vary by filled or unfilled resin-system construction.
Applications / Suitable for
- Coloring epoxy potting and casting systems
- Coloring polyurethane encapsulation systems
- Modification of electrical insulation compounds
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | One-part color concentrate | N/A | As supplied |
| Color | Black | N/A | DS-1832 |
| Pigment concentration | 18 | % | Product identification |
| Unfilled-system addition | 3 to 5 | parts by weight | Per 100 parts base epoxy resin or urethane curative |
| Total-system addition | 2 to 4 | % by weight | Unfilled total mixed system |
| Filled-system addition | 2 to 3 | parts by weight | Per 100 parts base resin or curative |
| Shelf life | 12 | months | Below 25°C in original sealed containers |