CONAP S-13
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- CE-1170 Conformal-Coating Reducing Solvent
- Viscosity Adjustment and Cleanup
- 27 deg C Flash Point
Product Description
CONAP® S-13 Reducing Solvent is a water-white aromatic hydrocarbon solvent used to adjust the viscosity of CONAP CE-1170 acrylic conformal coating. The material is added at room temperature to maintain the relationship between coating solids and viscosity or to compensate for evaporative losses. It may also be used as a compatible cleanup solvent within the documented coating process. Typical as-supplied properties include a specific gravity of 0.85 to 0.88 at 20°C and a closed-cup flash point of 27°C.
Key features
- CE-1170 viscosity adjustment: The solvent is specified for CONAP CE-1170 acrylic conformal coating.
- Process consistency: It supports correction of viscosity and evaporative losses while maintaining solids-to-viscosity balance.
- Controlled solvent properties: Typical specific gravity is 0.85 to 0.88 with a 27°C flash point.
Applications / Suitable for
- Reducing CONAP CE-1170 conformal coating
- Compensating for evaporative solvent loss
- Compatible cleanup in CE-1170 coating processes
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Reducing solvent | N/A | As supplied |
| Composition | Aromatic hydrocarbon solvent | N/A | Product description |
| Color | Water-white | N/A | At 25°C |
| Specific gravity | 0.85 to 0.88 | N/A | At 20°C |
| Flash point | 27 | °C | Closed cup |
| Shelf life | 12 | months | Below 25°C in original sealed containers |