CONAPOXY FR-1047
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Curative-Selectable Potting Window
- Low-Exotherm Electrical Casting
- Flame-Retardant Filled Resin
Product Description
CONAPOXY FR-1047 Epoxy Resin System is a mineral-filled, black epoxy resin used with a selected CONACURE hardener for flame-retardant potting and casting. Different hardeners provide different mixed viscosities, gel times, flexibility levels and cured properties, so the resin requires a compatible curative to form a complete system. Its filled formulation provides low-exotherm processing for electrical insulation applications. The system is used to pot and encapsulate modules, transformers, coils and strain-sensitive electrical or electronic devices with the appropriate hardener, mix ratio and cure schedule.
Key features
- Selectable CONACURE Hardeners: provides curative-dependent viscosity, gel time, flexibility and cured-property options
- Low-Exotherm Filled Resin: provides a low-exotherm profile for potting and casting
- Electrical Potting System: is used for modules, transformers, coils and strain-sensitive electrical devices
Applications
Potting and encapsulation of modules, transformers, coils and strain-sensitive electrical or electronic devices.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Values apply to CONAPOXY FR-1047 Black Resin before addition of a CONACURE hardener.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Black | FR-1047 resin, as supplied | |
| Viscosity | 58,000 | cP | FR-1047 resin at 25 deg C |
| Specific gravity | 1.7 | FR-1047 resin at 25 deg C | |
| Flash point | >94 (>201) | deg C (deg F) | FR-1047 resin; ASTM D93 |
| Shelf life | 12 | months | Original sealed container; dry storage below 25 deg C, out of direct sunlight |