CONATHANE EN-2521
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Filled Polyurethane Encapsulant for Modules
- 65 to 130 deg C Service Range
- 39% Cured Elongation
Product Description
CONATHANE® EN-2521 Polyurethane Encapsulant is a two-component, filled polyurethane potting and encapsulation system for modules, strain-sensitive circuitry, transformers, and coils. The system is recommended for applications requiring performance from -65°C to 130°C and is documented for low exotherm, low cure stress, low shrinkage, electrical insulation, and thermal-shock resistance. Published data identify a 17:100 mix ratio by weight, 4,000 cP initial mixed viscosity, and room-temperature or heat-cure schedules. Typical cured properties include Shore A 90 hardness, 39% elongation, and 585 V/mil dielectric strength.
Key features
- Wide temperature performance: The documented application range is -65°C to 130°C.
- Low-stress filled system: The polyurethane is documented for low exotherm, low shrinkage, and thermal-shock resistance.
- Electrical insulation: Typical cured dielectric strength is 585 V/mil.
Applications / Suitable for
- Electronic modules
- Strain-sensitive circuitry
- Transformers and coils
TDS, SDS & Technical Documents
- CONATHANE® EN-2521 Polyurethane Encapsulant Technical Data Sheet
- CONATHANE® EN-2521B Polyurethane Encapsulant Safety Data Sheet
- CONATHANE® EN-2521A Polyurethane Encapsulant Safety Data Sheet
- ELANTAS PDG Brochure - Formulated Resins Conformal Coatings
- ELANTAS PDG Brochure - Electronics and Electrical Applications
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Two-component filled polyurethane | N/A | System |
| Color | Brown or black | N/A | Available configurations |
| Mix ratio | 17:100 | parts by weight | Part A : Part B |
| Initial mixed viscosity | 4,000 | cP | Published portfolio value |
| Cure option | 7 | days | At 25°C |
| Cure option | 16 | h | At 80°C |
As-supplied / before-processing properties
Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Two-component filled polyurethane | N/A | System |
| Color | Brown or black | N/A | Available configurations |
| Mix ratio | 17:100 | parts by weight | Part A : Part B |
| Initial mixed viscosity | 4,000 | cP | Published portfolio value |
| Cure option | 7 | days | At 25°C |
| Cure option | 16 | h | At 80°C |