CONATHANE PR-1167
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Single-Component Polyurethane Primer for Cured Polyurethane
- May Be Applied by Spray
- 75 cP Application Viscosity
Product Description
CONAP® PR-1167 Polyurethane Primer is a single-component, solvent-borne isocyanate prepolymer primer for bonding liquid polyurethane molding and potting compounds to difficult substrates. Documented substrates include cured polyurethane, neoprene rubber, and cadmium-plated metals. The light-amber primer may be applied by spray, dip, or brush and is allowed to air dry for one to two hours or until tack-free before the polyurethane is introduced. Typical as-supplied properties include 75 cP viscosity, 58% solids content, and 1.02 specific gravity at 25°C.
Key features
- Polyurethane bonding primer: The primer is used with liquid polyurethane molding and potting compounds.
- Multiple application methods: It may be applied by spray, dip, or brush.
- Controlled as-supplied properties: Typical viscosity is 75 cP with 58% solids content.
Applications / Suitable for
- Bonding polyurethane compounds to cured polyurethane
- Priming neoprene rubber
- Priming cadmium-plated metals
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Single-component primer | N/A | As supplied |
| Color | Light amber | N/A | As supplied |
| Viscosity | 75 | cP | At 25°C |
| Solids content | 58 | % | 135°C for 45 min |
| Specific gravity | 1.02 | N/A | At 25°C |
| Flash point | 27 | °C | ASTM D93 |
| Air-dry time | 1 to 2 | h | Or until tack-free |
| Shelf life | 12 | months | At or below 25°C in original sealed containers |