COOLTHERM 6712

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM 6712

Main features

Product Description

Circalok™ 6712 is a two-component, low-viscosity, solvent-free silicone encapsulant that cures at room temperature to form an elastomeric, stress-relieving rubber with excellent electrical insulation and high-temperature performance. It is designed for potting and encapsulating densely packed electronic components and for producing flexible molds. The material offers a typical viscosity of 7,250 cP, continuous service temperatures from -55 to 205 °C, intermittent exposure up to 300 °C, and low linear shrinkage after cure.

Key Features

  • Low-viscosity, solvent-free silicone for room-temperature curing and encapsulation of densely packed assemblies.
  • Outstanding electrical insulation with high dielectric strength, high volume resistivity, and stable dielectric properties.
  • Wide service temperature capability with continuous operation from -55 to 205 °C and intermittent exposure up to 300 °C.

Applications / Suitable for

  • Potting electronic components
  • Encapsulating densely packed electronic assemblies
  • Manufacturing flexible molds
Product Family

COOLTHERM 6712

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
White
Specific Gravity Specific Gravity
1.16
Physical Properties
Viscosity Viscosity
7250 mPa.s
Mechanical Properties
Elongation Elongation
180 %
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.7 W/m.K
Electrical Properties
Dielectric Strength Dielectric Strength
0.5 kV/mm
Volume Resistivity Volume Resistivity
10^14 Ohms⋅cm

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical uncured properties before catalyst addition and curing.

Property Value Unit Method / Condition
Product type Two-component silicone — Solvent-free encapsulant
Specific gravity 1.16 — 25 °C
Viscosity 7,250 cP 25 °C
Standard color White — Black also available
Shelf life 6 months Closed containers from shipment date
Technical Properties

After-Processing / Final-State Properties

Typical cured properties after catalyst addition and curing.

Property Value Unit Method / Condition
Tensile strength 340 psi 25 °C
Elongation at yield 180 % Typical
Hardness 35 Shore A Typical
Linear shrinkage 0.002 in/in Typical
Continuous service temperature -55 to 205 °C Typical
Intermittent service temperature -100 to 300 °C Typical
Thermal conductivity 2.4 BTU·in/ft²·hr·°F Typical
Volume resistivity 1 × 1014 Ω·cm 25 °C
Dielectric constant 3.6 — 25 °C, 100 kHz
Dielectric strength 500 V/mil Typical