CYBERBOND 2008
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Fast EPDM and Elastomer Bonding
- Low-Viscosity Close-Fit Wetting
- Single-Component Rapid Assembly
Product Description
Cyberbond 2008 combines a low-viscosity ethyl cyanoacrylate format with fast bonding for elastomers and plastics. The product is specifically used for EPDM bonding, giving it a focused role where a thin instant adhesive is needed to wet close-fitting rubber interfaces. Its no-mix format supports controlled dispensing and rapid assembly. Cyberbond 2008 is used for small, well-fitted joints where low viscosity and fast set behavior are more important than gap filling. It is intended for fast elastomer and plastic component bonding.
Key features
- EPDM and elastomer bonding: The adhesive is specifically used for EPDM and other elastomer applications.
- Low-viscosity interface wetting: The thin liquid format supports close-fitting rubber and plastic joints.
- Rapid one-part assembly: No resin-to-hardener mixing is required before fast bonding operations.
Applications / Suitable for
- EPDM component bonding
- Elastomer and rubber assemblies
- Close-fitting plastic joints
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
As-supplied and application characteristics for the one-component adhesive. Values are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Technology / base | Ethyl cyanoacrylate | One-component adhesive | |
| Physical form | Low-viscosity liquid | As supplied | |
| Cure mechanism | Humidity initiated | Cyanoacrylate cure | |
| Primary material context | Elastomers and plastics | Bonding scope | |
| Specific substrate context | EPDM | Application material |