CYBERBOND 2241
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Toughened Structural Bonding
- Metal, Plastic, and Rubber Bonding
- Up to 140 deg C Service
Product Description
CYBERBOND 2241 is a black, fast-setting, rubber-toughened ethyl cyanoacrylate adhesive from the xtraflex Series. Designed as a partly flexible adhesive, it provides shock absorbence and high temperature resistance, making it excellent for dynamic, temperature-loaded bonds and combination bonding of metals to rubber or plastics.
Key features
- Rubber toughened: Offers partial flexibility to absorb shocks and withstand dynamic loads.
- High temperature resistance: Maintains performance across a broad service temperature range of -55 to 140°C.
- Fast bonding performance: Features quick setting times, such as 6-16 seconds on EPDM and 7-13 seconds on ABS plastics.
Applications / Suitable for
- Combination bonding of metal to rubber.
- Combination bonding of metal to plastic.
- Applications requiring shock absorbence and dynamic load resistance.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Uncured monomer properties of CYBERBOND 2241.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base Compound | Ethyl-2-cyanoacrylate | - | - |
| Appearance | Black | - | - |
| Density | 1.06 | g/cm³ | at 20°C |
| Viscosity | 2000-4000 | cps | cone-plate, @ 20°C @ 160 rpm |
| Setting Time (Metal/Steel) | 30-90 | seconds | - |
| Setting Time (EPDM) | 6-16 | seconds | - |
| Setting Time (Plastic/ABS) | 7-13 | seconds | - |
After-processing / final-state properties
Physical properties of cured CYBERBOND 2241 polymer.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service Temperature Range | -55 to 140 | °C | - |
| Strength (Steel) | 18 to 28 | N/mm² | - |
| Strength (NBR-rubber) | 5 to 12 | N/mm² | Material failure |