CYBERBOND 6020
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Targeted Cyanoacrylate Residue Removal
- Low-Viscosity Surface Treatment
- Repeat-Application or Soak Removal
Product Description
Cyberbond UNDO 6020 is a nitromethane-based liquid remover for softening and dissolving cyanoacrylate adhesive in unwanted areas. The colorless, low-viscosity material can be applied to residue on compatible metal, plastic, and rubber surfaces, then allowed to work for several minutes before wiping or cleaning. Heavier deposits may require repeated application, while bonded parts may require extended soaking. The product has a typical viscosity of 1 cP and a specific gravity of 1.1 g/cm^3. Some plastics and other materials may be adversely affected.
Key features
- Cyanoacrylate residue removal: The liquid softens and dissolves unwanted cyanoacrylate adhesive.
- Low-viscosity application: The 1 cP remover can reach residue on compatible metal, plastic, and rubber surfaces.
- Wipe or soak processing: Removal can use several-minute treatment, repeated application, or extended soaking for bonded parts.
Applications / Suitable for
- Removing cyanoacrylate residue from compatible metal surfaces
- Softening cyanoacrylate on compatible plastic and rubber surfaces
- Separating bonded parts through extended soaking where appropriate
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical liquid properties for the cyanoacrylate remover; values are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base compound | Nitromethane | Liquid | |
| Appearance | Colorless liquid | As supplied | |
| Viscosity | 1 | cP | Typical liquid property |
| Specific gravity | 1.1 | g/cm^3 | Typical liquid property |
| Flash point | 96 | deg C | As supplied |
| Boiling point | 214 | deg F | As supplied |
| Shelf life | 18 | months | Unopened |