DK15EG-05 Black Insulating Coating Powder
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- DK15EG-05 Coating Powder
- Black, insulating, epoxy based
- Gasohol resistant, for automotive fuel pump motor armatures
Product Description
DK15EG-05 Black is an epoxy based coating powder developed for the insulation of motor armatures and stators. It offers cut-through temperature resistance and is flex-fuel (unleaded gasoline and methanol) resistant. DK15EG-05 Black is designed to be applied by an electrostatic fluid bed process, offering a fast cure in an induction coil curing process. Particle size is tailored to provide low dusting levels.
DK15EG-05 is flex-fuel (gasohol, gasoline/ethanol blend) resistant, Class F-rated epoxy powder coating for slot insulation of automotive fuel pump motor armatures and stators. It works extremely well for both AC and DC electric motors, including those used for in-tank fuel pumps. The coating provides superior flex fuel resistance, edge coverage, and high impact strength. High cut through temperature serves to protect the motor even at high operating temperatures. DK15EG-05 is designed for electrostatic fluid bed application, and DK15EG-05 is tested and qualified for UL EIS 1446 155°C (Class F) rating.
DK15EG-05 is available in both black and green color. It is black in color, though DK15EG-05 Green is the green color version of DK15EG-05 Black. Both versions have been used for over 20 years by major manufacturers of automotive enclosures, fuel pumps, windshield wipers, seat adjusters, and other, DK15EG-05 provides a smooth surface appearance with high edge coverage. Particle size is optimized for high productivity on an electrostatic fluidized bed coating process including Braun Sondermaschinen.
Advantages of DK15EG-05 for Slot Insulation
- Flex-fuel resistant, suitable for exposure to automotive fluids
- A high pickup powder, it provides high productivity on Braun Sondermaschinen and other electrostatic fluidized bed machines
- Permits the use of more copper in the slots allowing for smaller, higher-power motors
- Reduced copper waste compared to slot liners since the winding does not need to go up and over the liner
- Excellent moisture resistance, even in high temperatures and corrosive conditions
- A high-productivity coating powder, used for decades in the manufacture of fuel pump assemblies
Typical applications and uses of DK15EG-05 Black or Green include:
- Slot Insulation of AC and DC Motor Armatures
- Slot Insulation of Stators
- Slot Insulation of Motor Armatures in Fuel Pump Motors
- It has also been tested successfully for hairpin coating of 400V electric motors
This product is no longer available. Some alternatives for armature and stator coating powders are:
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Other Properties
Mechanical Properties
Additional Information
{tab=Pricing & Availability}
|
Pricing and Volume Price Breaks for {product_name} are available by contacting us. You cannot order this product directly online. KRAYDEN lists all its prices without taxes, shipping payment charges or discounts. KRAYDEN has warehouses and ships from both Canada and the Netherlands, and if your shipping address is one of these two countries, applicable taxes will be applied. If your shipping address is to the United States, we request your company’s Employer Identification Number (EIN) or Tax Identification Number (TIN). This is a unique 9-digit number assigned by the IRS and is required for all cross-border shipments. Failure to provide this number could result in delays to your order. If your shipping address is within the EU, but outside the Netherlands, then we are required to request your company's Value Added Tax (VAT, BTW, MwSt) number to be able to ship the goods tax-free. For all other countries, no taxes are levied on your orders. Minimum Order Quantity for {product_name}The minimum order quantity for this package size is {min_order_quantity} {product_unit}(s). Shipping Charges for {product_name}All prices shown are ex-works KRAYDEN, but during the checkout process, you will be given several shipping options including Canada Post, TNT, UPS or the choice of using your own freight forwarder. Depending on your shipping address, the shipping charges will be calculated as follows:
Payment option for {product_name}During the checkout process, you will be presented with several payment options including:
Availability for {product_name}To the right of the product is a small icon that lets you know the availability and leadtime of the product. This leadtime is the time to ship the product and delivery times vary based on the method of delivery you select at the time you place your order. Contact us if anything is unclear or you need more assistance. |
{tab=Technical Specifications}
Technical Datasheets for {product_name}TDS (English) |
{tab=Competitive Crossovers}
#shortdesc
|
Please see the section above for a list of Competitive Brands that {product_name} competes against. |
{tab=Videos & Other Media}
|
Please visit or subscribe to our YouTube Channel. See this video that shows the difference between a good and a bad fluidized epoxy coating powder bed. |
{tab=Product Reviews}
|
{review} |
{tab=Packaging Details}
|
The following information is specifically related to each unit of measure of {product_name}. If you which to compare this to other product sizes, click on the respective product from the list above and check here for values specific to that product. These values are taken from our internal database and are used in the calculation of the gross weight and packaging dimensions of the goods during shipping. You can use these values to to approximate delivery charges using your own carrier. Each unit of {product_name} has the following:
|
{tab=View Blogs & Forum}
| KRAYDEN is different. Unlike other business to business enterprises, we encourage our customers to discuss, critique, and otherwise comment on the products we offer. Get more technical information, read detailed posts, and see what customers have to say about about {product_name} on our Corporate Blog and Forum. |
{/tabs}