CS-783 | Methacrylated Epoxy Functional Hybrid Cyclosiloxane
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Low viscosity
- Dual cure mechanism
- Multifunctional
Product Description
DMI CS-783 is a methacrylated, epoxy-functional hybrid cyclosiloxane monomer engineered to enhance adhesion and compatibility in advanced resin systems. Its unique structure allows participation in both free-radical polymerization and epoxy curing mechanisms, offering broad versatility for formulating high-performance adhesives, coatings, and composite materials.
Used primarily as an adhesion promoter for mold compounds, metal surfaces, and polyimides, DMI CS-783 improves interfacial bonding without sacrificing processing ease. Additionally, it serves as a multifunctional diluent, reducing viscosity and enhancing flow properties across a wide range of resin systems. Soluble in most common resins, DMI CS-783 simplifies formulation without compromising performance.
Applications
- Adhesion promoter for mold compounds, metals, and polyimide surfaces
- Reactive diluent for epoxy, hybrid, and UV-curable systems
- Formulations requiring dual-cure compatibility (free-radical and epoxy cures)
- B-staged and hybrid adhesives, coatings, and composites
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
Recommended Formulation Use
- CS-783 is recommended for use as an adhesion promoter to mold compounds and metal substrates. Typical addition levels are 1-5% of the total resin. CS-783 can also be used for standard epoxy curatives, catalysts, B-staged and/or hybrid adhesives.
|
Property |
Value |
Unit |
|
Physical and Chemical Properties |
||
|
Epoxy functionality |
2-4 |
- |
|
Methacrylate functionality |
1-2 |
- |
|
Average epoxy equivalent weight |
261 |
- |