MM281 | Maleimide adhesion promoter Additive
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Adhesion promoter
- Flexible aliphatic backbone
- Long Alkyl chain
Product Description
MM-281 is a long chain maleimide terminated carboxylic acid. It is a useful intermediate for the synthesis of ester and amide linked thermoset monomers. The long alkyl chain provides flexibility and hydrophobicity
ΜΜ-281 has a flexible aliphatic backbone and maleimide and carboxylic acid functional groups that aid in adhesion promotion in free-radical or in epoxy/(meth)Acrylate hybrid adhesives . It is recommended for use as an intermediate for maleimide functional resins and the main difference with the seemingly identical MM-211 is the twice as long alkyl chain.