DOWSIL 280A
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Tack/Adhesion up to 260 deg C
- Solvent-Based Peroxide-Cure Silicone PSA
- Masking, Plating, and Splicing Tapes
Product Description
DOWSIL™ 280A Adhesive is a solvent-based silicone pressure-sensitive adhesive formulated for masking, plating, and splicing tape constructions. The peroxide-cure adhesive combines good tack with adhesion performance at temperatures up to 260°C (500°F), making it relevant for tape applications that require temporary or process-stage attachment during elevated-temperature operations. Its reported nonvolatile content of 57%, viscosity of 38,900 mPa·s, and specific gravity of 0.98 at 25°C provide useful selection data for coating and converting evaluation.
Key features
- High-temperature adhesion: Provides good tack and adhesion at temperatures up to 260°C (500°F).
- Silicone pressure-sensitive adhesive: Solvent-based, peroxide-cure formulation for specialty tape constructions.
- High-tack application profile: Suitable for tape applications requiring a balance of properties with emphasis on tack.
Applications / Suitable for
- Masking tapes
- Plating tapes
- Splicing tapes
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical properties of DOWSIL™ 280A Adhesive as supplied.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Nonvolatile content | 57 | % | Typical value |
| Viscosity | 38,900 | mPa·s | Typical value |
| Specific gravity | 0.98 | — | At 25°C |
| Flash point | 27 | °C | Closed cup |
| Shelf life | 270 | days |