DOWSIL™ EA-4700 CV Adhesive
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Two-part system
- Fast curing options
- Controlled volatility
Product Description
DOWSIL™ EA-4700 CV Adhesive is a two-part, fast room temperature cure adhesive designed for critical adhesive and sealing performance. It features controlled silicone volatility and maintains high temperature stability after curing. With a dispensable formulation for easy application using standard equipment, it provides good sealing against environmental conditions.
Product Key Features
- Two-Part System - features a 1:1 mix ratio by weight or volume, making it easy to dispense and mix.
- Fast Curing Options - offers a fast cure at room temperature, reaching hardness completion in 2 hours at 25°C, or can be heat-accelerated for faster processing.
- Controlled Volatility - maintains a low volatile siloxane content (D4-D10) of 130 ppm.
- Robust Mechanical Profile - cures to deliver a JIS Type A hardness of 19, a tensile strength of 3.7 MPa, and an impressive elongation of 630%.
- Environmental Stability - delivers stable performance under typical operational environments, including exposure to 150°C, thermal shock, and 85°C/85% relative humidity.
Applications
This adhesive fits a variety of automotive applications requiring durable adhesion to typical substrates used in automotive electronics, such as aluminum, PBT, and PPS.
- Automotive Electronics: Ideal for electronics control units, sensor modules, and battery pack applications.
- Component Assembly: Used effectively for lid sealing, base plate attaching, and connector sealing where reliable adhesion is necessary.
- Gasketing: Provides reliable gasketing with durable sealing against the environment.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Electrical Properties
Additional Information
DOWSIL™ EA-4700 CV Adhesive
DOWSIL™ EA-4700 CV Adhesive is a high-performance, two-part silicone structural adhesive engineered to deliver exceptionally fast room temperature curing or rapid heat-accelerated bonding. Formulated with an advanced addition-cure mechanism, it cross-links uniformly through deep sections or complete component confinement without releasing volatile by-products. This adhesive features controlled silicone volatility with reduced volatile siloxane content (D4-D10) and is highly specialized to provide a durable, fluid-tight environmental seal. Its robust, tough matrix offers excellent stress relief and reliable performance for sensitive automotive electronics exposed to extreme high-temperature stability up to 150°C, severe thermal shock, and high humidity aging environments.
Typical engineering values only. Adhesion builds reliably after hardness completion; cure parameters can be accelerated through targeted heating lines.
Key Features
- Two-part thixotropic paste offers a symmetrical 1:1 mix ratio by volume or weight for easy processing.
- Addition-cure chemistry yields zero volatile cross-linking by-products, preventing shrinkage stress.
- Enables rapid deep-section solidification and uniform curing through totally confined substrate pockets.
- Controlled silicone volatility limits volatile siloxane outgassing (D4-D10) to 130 ppm to shield electronics.
- Maintains high environmental sealing stability continuously at 150°C, thermal shock, and 85°C / 85% RH.
- Establishes excellent unprimed primerless adhesion to typical plastics and metals used in automotive assemblies.
Processing Summary
Process Notes
- Realizes a 12-month shelf life from production date when held in cold storage below 30°C.
- Keep containers tightly closed in original packaging to completely block moisture and contamination.
- Formulated to prevent heavy settling, but stir thoroughly if stored for several months.
- Always verify expiration dates and specific storage instructions listed on the batch labels.
- Clean substrate surfaces using Dow OS fluids, naphtha, mineral spirits, or methyl ethyl ketone (MEK).
- Do not rely on acetone or isopropyl alcohol (IPA) alone, as they fail to adequately clear manufacturing oils.
- Introduce fine mechanical abrasion to maximize active bonding contact surface area.
- Use plasma exposure or chemical etching to establish a reactive face on Teflon, PE, or PP lines.
- Avoid contact with organotin catalysts, tin-catalyzed silicone rubbers, and sulfur-containing materials.
- Prevent exposure to polysulfides, polysulfones, unsaturated hydrocarbon plasticizers, or solder flux residues.
- Tacky or liquid product remaining at the joint boundary layer indicates active chemical cure inhibition.
- Run lab-scale compatibility evaluations to confirm component material compliance before line setups.
- Utilize an engineered static mixer nozzle for manual cart or automated meter/mix dispense setups.
- Automated airless dispense equipment is ideal to minimize or bypass separate vacuum de-airing cycles.
- If de-airing is needed to eliminate joint voids, apply a vacuum profile of >203 mm Hg for 10 minutes.
- Mate substrate assemblies quickly after extrusion within the specified 20-minute working window.
Engineering Data for DOWSIL™ EA-4700 CV
Uncured Physical & Dispensing Properties
| Property Parameter | Part A Value | Part B Value | Mixed | Test Condition |
|---|---|---|---|---|
| Appearance / Color | White paste | Black paste | Gray non-slump paste | CTM 0176 B |
| Viscosity at 10 s⁻¹ | 24 Pa·s | 18 Pa·s | 27 Pa·s | Mixed viscosity / CTM 1094 R |
| Thixotropic Index | — | 3.8 | Ratio 1 s⁻¹ / 10 s⁻¹ mixed / CTM 1094 R | |
| Working Time @ 25°C | — | 20 minutes | CTM 1094 R | |
| Cured Density at 25°C | — | 1.16 g/cm³ | CTM 0022 B | |
Cured Electrical & Mechanical Characteristics
Physical parameters evaluated following an ambient room temperature cure profile of 3 days at 23°C / 25°C.
| Mechanical or Electrical Property | Typical Engineering Value | Test Method Standard Basis |
|---|---|---|
| Durometer Hardness | 19 | JIS Type A / CTM 0099 M |
| Tensile Strength | 3.7 MPa | CTM 0137AAH |
| Elongation | 630 % | CTM 0137ABH |
| Dielectric Strength | 25 kV/mm | JIS K 6249 |
| Volume Resistivity (Non-Dried) | 1.5E+15 ohm·cm | JIS K 6249 |
| Dielectric Constant / Dissipation Factor | 3.2 / 1.8E-03 | 1 MHz / JIS K 6249 |
| UL Flammability Classification | 94-HB | Underwriters Laboratories standard safety rating |
Unprimed Adhesion Lap Shear Strength (JIS K 6249)
| Substrate Base Material | Cure Profile Schedule | Lap Shear Value | Failure Mode Result |
|---|---|---|---|
| Aluminum (Anodized A5052P) | 2 hours @ 25°C | 1.2 MPa | Early tracking build |
| 8 hours @ 25°C | 2.2 MPa | Cohesive Failure (100% CF) | |
| 24 hours @ 25°C | 3.1 MPa | Cohesive Failure (100% CF) | |
| 72 hours @ 25°C | 3.9 MPa | Cohesive Failure (100% CF) | |
| 5 minutes @ 80°C | 1.3 MPa | Cohesive Failure (100% CF) | |
| PBT Plastic (Unfilled) | 2 hours @ 25°C | 1.8 MPa | Early tracking build |
| 8 hours @ 25°C | 2.0 MPa | Cohesive Failure (100% CF) | |
| 24 hours @ 25°C | 2.1 MPa | Cohesive Failure (100% CF) | |
| 72 hours @ 25°C | 2.7 MPa | Cohesive Failure (100% CF) | |
| 5 minutes @ 80°C | 1.5 MPa | Cohesive Failure (100% CF) |
Where DOWSIL™ EA-4700 CV Fits
- Durable lid sealing and base plate attaching.
- Forms a tough, flexible, fluid-tight gasketing layer.
- Maintains high environmental protection on Aluminum and PBT plastic.
- Reliable structural gasketing for heavy EV battery packs.
- Critical sealing performance across electronic sensor modules.
- Withstands severe continuous vibration and thermal shock cycles.
Connector Sealing & Confinement- Seals wires and terminals inside fully confined configurations.
- Controlled siloxanes limit outgassing to protect contact points.
- 630% ultimate elongation absorbs joint stresses under CTE mismatch.
Standard Packaging & Technical Help
- Available as matching Part A (White) and Part B (Black) component kit pairs.
- Supplied across multiple standard industrial protective packaging sizes.
- Containers must be kept tightly closed and stored in cold storage at all times.
- Please contact Dow or your local distributor to confirm specific packet net weights.
- Configuring targeted heat profiles to enable fast 5-minute production bonding lines.
- Auditing shop floor environments to prevent addition-cure catalyst inhibition risks.
- Calibrating dual-fluid pump variables to ensure exact 1:1 mixing by weight or volume.
- Assisting with lab-scale substrate qualification trials to verify cohesive fail limits.
Tips and Troubleshooting
| Issue | Recommended Action |
|---|---|
| Light-colored streaks or marble patterning visible in the compound bead |
|
| Adhesive fails to cross-link properly, remaining liquid or tacky at the boundary |
|
| Occurrence of macro-voids or bubble clusters within cured joint channels |
|