DOWSIL SE1714

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL SE1714

Main features

  • One-Part No-Mix Bonding
  • 30-Minute 150 deg C Cure
  • 1,030 psi Cured Tensile Strength

Product Description

DOWSIL™ SE 1714 Adhesive is a one-part, black or beige, flowable addition-cure silicone adhesive and sealant for electronics and automotive assemblies. The ready-to-use material requires no mixing and is heat cured above 100°C, with a typical cure condition of 30 minutes at 150°C. Documented applications include sealing lids and housings for electronic control units and power modules, fixing printed circuit-board and system assemblies, and reinforcing connector components. Typical cured properties include Shore A 65 hardness, 1,030 psi tensile strength, 250% elongation, and a specific gravity of 1.3 at 25°C.

Key features

  • One-part flowable adhesive: The ready-to-use material can flow, fill, or self-level after dispensing.
  • Heat-cure processing: A typical cure condition is 30 minutes at 150°C.
  • Strong cured elastomer: Typical data include 1,030 psi tensile strength and 250% elongation.

Applications / Suitable for

  • Sealing lids and housings for ECUs and power modules
  • Fixing PCB and system assemblies
  • Reinforcing or fixing connector components
Product Family

DOWSIL SE1714

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form One-part flowable adhesive / sealant N/A As supplied
Color Black or beige N/A As supplied
Cure type Addition cure N/A Heat cure above 100°C
Typical cure 30 min At 150°C
Technical properties

After-processing / final-state properties

Typical cured, installed, or in-use values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Specific gravity 1.3 N/A At 25°C
Hardness 65 Shore A Typical cured value
Tensile strength 1,030 psi Typical cured value
Elongation 250 % Typical cured value