DYMAX 3019
Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other
Main features
- Fast UV/Visible-Light Plastic Bonding
- Moisture-Resistant Clear Bond Lines
- Fluorescent In-Line Inspection
Product Description
Dymax Ultra Light-Weld 3019 Series Moisture-Resistant Adhesives are UV- and visible-light-curable adhesives for fast bonding of flexible and rigid plastic substrates. The 100% reactive-solids, solvent-free formulations form clear bond lines on materials including polycarbonate, PVC, polyurethane, PET, PETG, polystyrene, and nylon. The series includes a nominal 450 mPa s 3019 liquid and a 25,000 mPa s 3019-GEL grade for different dispensing requirements. After cure, typical series properties include Shore D55 hardness, 1,700 psi tensile strength, and 170% elongation at break. The adhesives also fluoresce under low-intensity 365 nm black light, supporting in-line inspection of dispensed and bonded areas.
Key features
- Fast light-activated bonding: UV or visible light develops bonds in seconds under validated exposure conditions.
- Liquid and gel viscosities: The series includes nominal 450 mPa s and 25,000 mPa s grades for different dispensing needs.
- Fluorescent inspection: The adhesive fluoresces under low-intensity 365 nm black light.
Applications / Suitable for
- Polycarbonate and PVC bonding
- Polyurethane, PET, and PETG bonding
- Polystyrene and nylon bonding
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Chemical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied properties for the 3019 Series; viscosity depends on grade.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Solvent content | None | 100% reactive solids | |
| Appearance | Clear to light amber | As supplied | |
| Refractive index | 1.48 | At 20 deg C | |
| Density | 1.05 | g/mL | Typical |
| 3019 viscosity | 450 | mPa s | Nominal; ASTM D1084 |
| 3019-GEL viscosity | 25,000 | mPa s | Nominal; ASTM D2556 |
| Shelf life | 12 | months | Unopened container |
| Storage temperature | 10 to 32 | deg C | Unopened container |
After-processing / final-state properties
Typical cured properties for the 3019 Series.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Durometer hardness | 55 | Shore D | Cured material |
| Tensile strength | 1,700 | psi | Cured material |
| Elongation at break | 170 | % | Cured material |
| Modulus of elasticity | 30,000 | psi | Cured material |
| Water absorption | 2.1 | % | 24 hours |
| Boiling-water absorption | 1.3 | % | 2 hours |
| Linear shrinkage | 3.0 | % | After cure |