DYMAX 628-VLV
Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other
Main features
- Close-Fitting Joint Wicking
- Post-Assembly Crack and Crevice Bonding
- Insulating Multi-Substrate Attachment
Product Description
Dymax 628-VLV Wicking Grade Structural Adhesive is a low-viscosity UV- and visible-light-curable urethane acrylate adhesive for wicking into close-fitting joints, cracks, and crevices. The 100% reactive-solids formulation reaches confined bond areas by capillary action before cure, supporting protective coating and structural bonding tasks. It bonds glass, metal, phenolic, filled nylon, ferrite, and ceramic within the supported substrate range. The cured material provides a hard structural bond and electrical insulation properties for compact electromechanical and industrial assemblies. Applications include post-assembly wicking, reinforcement of close-fitting surfaces, and bonding small components where adhesive flow into narrow gaps is useful.
Key features
- Post-assembly wicking: Low viscosity allows the adhesive to enter close-fitting joints, cracks, and crevices.
- Reactive-solids formulation: The 100% reactive-solids chemistry cures without a solvent-evaporation stage.
- Insulating structural bond: The cured material combines structural attachment with dielectric properties.
Applications / Suitable for
- Protective coating of close-fitting surfaces
- Wicking into cracks and crevices
- Bonding glass, metal, phenolic, filled nylon, ferrite, and ceramic
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Chemical Properties
Additional Information
As-supplied / before-processing properties
Exact-product as-supplied characteristics relevant to capillary wicking and light-cure processing.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Reactive solids | 100 | % | As supplied |
| Chemistry | Urethane acrylate | As supplied | |
| Viscosity class | Low | Wicking grade | |
| Flow behavior | Capillary wicking | Close-fitting joints, cracks, and crevices | |
| Cure activation | UV and visible light | Exposed adhesive |
After-processing / final-state properties
Exact-product final-state characteristics relevant to confined structural joints.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Cured bond character | Hard structural bond | After light cure | |
| Electrical behavior | Electrically insulating / dielectric | Cured adhesive | |
| Bonded substrate scope | Glass; metal; phenolic; filled nylon; ferrite; ceramic | Within the listed substrate scope | |
| Final joint geometry | Close-fitting joints and confined gaps | Post-assembly wicking |