DYMAX 706
Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other
Main features
- Cooling-Hole Process Protection
- Aggressive Metal-Processing Resistance
- Low-Ash Thermal Removal
Product Description
Dymax SpeedMask 706 Maskant is a UV- and visible-light-curable process maskant for turbine-component and high-temperature metal processing. The material protects selected areas during acid stripping, air plasma spray, and machining, including cooling-hole protection on supported nickel superalloys and high-temperature steel. After cure, the mask forms a durable temporary barrier intended for demanding process exposure and controlled removal. The product is selected where a removable mask must remain in place through aggressive operations while limiting residue after the stated removal sequence. Its application focus is process protection rather than permanent coating or structural bonding.
Key features
- Turbine-feature protection: The maskant is used to protect cooling holes and selected component areas during processing.
- Aggressive-process resistance: Supported operations include acid stripping, air plasma spray, and machining.
- Controlled burn-off removal: The cured mask is intended for removal by the documented thermal process with low residual ash.
Applications / Suitable for
- Acid stripping
- Air plasma spray and machining
- Cooling-hole protection on turbine components
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Mechanical Properties
Chemical Properties
Physical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
As-supplied and pre-processing characteristics for application to high-temperature metal components.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Removable process maskant | As supplied | |
| Cure activation | UV and visible light | Applied maskant | |
| Target materials | Nickel superalloys; high-temperature steel | Recommended substrate scope | |
| Protected features | Cooling holes and selected component areas | Before aggressive processing | |
| Process preparation role | Temporary masking barrier | Before acid, spray, or machining exposure |
After-processing / final-state properties
Final cured-mask characteristics during processing and removal.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Cured function | Durable temporary process barrier | After light cure | |
| Process exposure scope | Acid stripping; air plasma spray; machining | Stated operations | |
| Removal method | Thermal burn-off | After processing | |
| Residue characteristic | Low residual ash | After the stated burn-off sequence | |
| Final application boundary | Temporary protection only | Not a permanent coating |