DYMAX 726-SC
Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other
Main features
- Visual See-Cure Verification
- Flexible Multi-Process Protection
- OMat and ISO Evaluation Scope
Product Description
Dymax SpeedMask 726-SC Maskant is a See-Cure process maskant that changes from blue before cure to pink after UV or visible light exposure. The color transition provides an immediate visual cue for cure progress while the material protects selected areas during plating, anodizing, gritting, shot peening, air plasma spray, and low-temperature powder coating. The cured mask is formulated to remain flexible across the stated process-temperature range and includes product-specific mechanical and qualification data. Its application scope also includes orthopedic implant protection where the exact ISO 10993-5 and Rolls-Royce OMat boundaries are retained.
Key features
- Blue-to-pink cure indication: See-Cure color change gives a visible cue from uncured blue to cured pink.
- Cross-process masking range: The material supports plating, peening, plasma spray, and low-temperature powder coating.
- Qualified application scope: The source package includes Rolls-Royce OMat and ISO 10993-5 evaluation context.
Applications / Suitable for
- Plating and anodizing
- Gritting, shot peening, and air plasma spray
- Low-temperature powder coating and orthopedic implant protection
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Chemical Properties
Physical Properties
Other Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Before-processing characteristics for placement and visual cure verification.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Physical form | Removable process maskant | As supplied | |
| Uncured color | Blue | Before light exposure | |
| Cure activation | UV and visible light | Applied maskant | |
| Cure indicator | Blue-to-pink color change | During light cure | |
| Process role | Temporary surface protection | Before the Stated operations |
After-processing / final-state properties
Cured-state characteristics, process scope, and product-specific evaluation boundaries.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Cured color | Pink | After sufficient light exposure | |
| Mechanical data scope | Shore D hardness and cured modulus | Product-specific cured-material evaluation | |
| Process-temperature behavior | Flexible within the stated range | During supported processing | |
| Qualification scope | Rolls-Royce OMat | Exact product scope | |
| Biological evaluation scope | ISO 10993-5 cytotoxicity evaluation | Within the stated test scope |