LOCTITE ECCOBOND FP4531

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond FP4531

Main features

  • Snap cure
  • Fast flow
  • Passes NASA outgassing

Product Description

LOCTITE® ECCOBOND FP4531 underfill is designed for flip chip on flex applications with a 1mil gap. It is a snap curable epoxy with fast flow that passes NASA outgassing standards.

LOCTITE® ECCOBOND FP4531 is 62% filled, offers a pretty long pot life and has limited impurities. Its snap cure schedule can vary based on customer's experience and application requirements.

 

Snap Cure Schedule

  • 7 minutes @ 160°C
Product Family

ECCOBOND FP4531

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 56 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life Pot Life
24 hours
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
161 °C
Thermal Conductivity Thermal Conductivity
0.61 W/m.K
Physical Properties
Viscosity Viscosity
10,000 mPa.s