ELANTAS AD-1161
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- PVC-to-Polyurethane Adhesion Priming
- Fast 30-Minute Air-Dry Step
- MIL-M-24041 QPL-Listed Primer
Product Description
CONAP AD-1161 Adhesive Primer is a light-amber, solvent-borne modified phenolic primer for bonding liquid polyurethane systems to prepared polyvinyl chloride surfaces. The 80 cP liquid can be applied by brush, spray, or roller, then air dried for 30 minutes at room temperature before polyurethane placement. Typical peel strength reaches 30 pli with EN-1554 and EN-1556 polyurethane systems on prepared PVC. The primer is QPL listed to MIL-M-24041 Category B, Type I and is supplied with a 12-month storage period at or below 25 deg C.
Key features
- PVC-Specific Adhesion Priming: The primer supports liquid polyurethane bonding to properly prepared polyvinyl chloride.
- 30-Minute Air Dry: A defined room-temperature air-dry step supports controlled polyurethane application.
- Qualified Primer Scope: QPL listing to MIL-M-24041 Category B, Type I preserves the exact qualification scope.
Applications / Suitable for
- Liquid polyurethane bonding to prepared PVC surfaces
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Other Properties
Additional Information
As-supplied / before-processing properties
As-supplied and processing characteristics used for material and process evaluation. Numerical values are typical unless otherwise identified.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Light amber | - | As supplied |
| Viscosity | 80 | cP | At 25 deg C |
| Solids content | 20 | % | Typical as supplied |
| Adjustment solvent | MEK | - | For application adjustment where required |
| Weight per gallon | 7.3 | lb/gal | Typical as supplied |
| Flash point | -9 | deg C | ASTM D93 |
| Shelf life | 12 | months | Stored at or below 25 deg C |