ELANTAS K-230
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics
Main features
- 100% Solids Epoxy Processing
- Room-Temperature Cure Route
- Bonding Across Thermal Expansion Differences
Product Description
EASYPOXY K-230 Two-Component Epoxy Adhesive is a 100% solids, room-temperature-curing epoxy adhesive and repair compound. The two-component system supports general-purpose bonding and repair, including assemblies that join materials with different coefficients of expansion. Its ambient cure route permits bonding without a required production oven, while the 100% solids formulation defines the supplied resin system. K-230 is suited to repair operations and bonded assemblies where dissimilar thermal expansion is an important material-selection factor and a two-part epoxy process is acceptable.
Key features
- 100% Solids Formulation: The adhesive is supplied as a two-component 100% solids epoxy system.
- Room-Temperature Cure: The material develops its bond through an ambient cure route.
- Dissimilar-Expansion Bonding: Applications include joining materials with different coefficients of expansion.
Applications / Suitable for
- General-purpose bonding
- Adhesive repair work
- Bonding materials with different coefficients of expansion
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Chemical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical properties of the individual components before mixing and curing.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 100,000 / 50,000 | cP | Part A Resin / Part B Hardener @ 25°C |
| Specific Gravity | 1.17 / 1.08 | — | Part A Resin / Part B Hardener @ 25°C |
| Mix Ratio | 100 : 45 | By weight | Part A : Part B |
| Work Life | 60 | minutes | 25°C / 77°F |
| VOC Content | <0.1 | % | ASTM D6053 |
After-processing / final-state properties
Typical cured properties of EASYPOXY® K-230.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shore Hardness | D80 | — | ASTM D2240, 25°C |
| Lap Shear Strength | 2,500 | psi | ASTM D1002, etched aluminum/aluminum, 25°C |
| Compressive Strength | 18,000 | psi | ASTM D695, 25°C |
| Flexural Strength | 10,000 | psi | ASTM D790, 25°C |
| Volume Resistivity | 4.0 × 10¹³ | ohm-cm | ASTM D257, 25°C |
| Thermal Conductivity | 0.2 | W/m·K | 25°C |