ENTHONE B3
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Four-Hour Ink Pot Life
- Controlled Heat-Cure Processing
- Faster Cure at Higher Temperature
Product Description
ENTHONE B-3 Catalyst is a heat-cure-only catalyst component for ENTHONE M-Series epoxy marking inks. It provides an average 4-hour pot life after the specified induction period, giving a defined processing window before the ink begins to solidify. Cure temperature must exceed 79 deg C, and higher temperatures shorten the required cure time within the published ink-film schedule. B-3 is used where permanent epoxy markings are processed through controlled thermal cure, including supported M-Series color packages and premeasured bi-pack configurations.
Key features
- Heat-Cure-Only Processing: B-3 is used exclusively with controlled thermal cure.
- Four-Hour Pot Life: The catalyzed ink has an average 4-hour working pot life after induction.
- Temperature-Responsive Cure: Higher cure temperatures reduce the required ink-film cure time.
Applications / Suitable for
- ENTHONE M-Series heat-cured marking inks
- M 0 N and M 9 N bi-pack configurations
- M 0 NC nonconductive black bi-pack configurations
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical catalyst and catalyzed-ink processing data. Final properties belong to the selected M-Series ink, catalyst ratio, and cure schedule.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Catalyst function | Basic heat-cure catalyst | - | ENTHONE M-Series epoxy marking inks |
| Cure mode | Heat only | - | B-3 catalyst |
| Average pot life | 4 | hr | Begins after induction period |
| Induction period | 30 | min | All standard catalysts, including B-3 |
| Required cure temperature | >79 | deg C | Above 175 deg F |
| Shelf life | 2 | years | All ENTHONE catalysts; from date of manufacture |