EPOCAST 1618

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

EPOCAST 1618

Main features

  • Pumpable Non-Flowing Placement
  • Fast 15-Minute Gel Time
  • Honeycomb Fastener Potting

Product Description

EPOCAST 1618 D/B Epoxy Syntactic is a low-density, self-extinguishing two-component epoxy syntactic compound for potting fasteners in honeycomb structures. The 1618-D resin and 1618-B hardener mix at 100:14 by weight and form a pumpable paste that can be extruded through a 1/8 in nozzle while remaining non-flowing after placement. The mixed system has a 15-minute gel time at 25 deg C and cures at room temperature or with a 52 deg C post-gel heat cycle. Typical cured compressive strength is 5.00 ksi at 25 deg C.

Key features

  • Pumpable non-flowing placement: The paste extrudes through a 1/8 in nozzle and remains in place after application.
  • Quick-setting system: The mixed material has a 15-minute gel time at 25 deg C.
  • Low-density cured compound: The mixed system has a typical specific gravity of 0.70.

Applications

  • Potting fasteners in honeycomb structures
Product Family

EPOCAST 1618

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
White
Physical Properties
Viscosity (Part B) Viscosity (Part B)
400 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-received values distinguish the resin, hardener, and mixed system.

Property Value Unit Method / condition
Color 1618-D white; 1618-B amber; mixed white - Visual
Specific gravity 1618-D 0.60; 1618-B 1.00; mixed 0.70 - ASTM D1622
Viscosity 1618-D paste; 1618-B 400; mixed paste cP ASTM D2196 at 25 deg C
Mix ratio by weight 100:14 - 1618-D resin:1618-B hardener
Gel time 15 min 57 g mass at 25 deg C; ASTM D2471
Shelf life 6 months Components unopened at 25 deg C
Technical properties

After-processing / final-state properties

Typical cured properties apply to the mixed EPOCAST 1618 D/B system.

Property Value Unit Method / condition
Cure schedule 24 h at room temperature; or room-temperature gel plus 5 h at 52 deg C - Typical cure
Compressive strength 5.00 ksi At 25 deg C; ASTM D695
Compressive modulus 350 ksi ASTM D695
Tensile lap shear 700 psi Aluminum-to-aluminum; ASTM D1002
Weight change in MIS-S-3136 Type III fluid 0.3 % 24-hour immersion at 25 deg C; ASTM D543
Weight change in Skydrol 500-A 0.6 % 24-hour immersion at 25 deg C; ASTM D543
Weight change in distilled water 1.5 % 24-hour immersion at 25 deg C; ASTM D543
Flammability Self-extinguishing - Typical cured material