EPOCAST 50-A1/9816

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

EPOCAST 50-A1/9816

Main features

  • Extended 65-Minute Gel Time
  • Solvent-Free Composite Laminating
  • Room-Temperature or Heat Cure

Product Description

EPOCAST 50-A1 Resin / Hardener 9816 Epoxy Laminating System is an unfilled, solvent-free two-component epoxy for composite structure manufacture, repair, and filament winding. The amber system mixes at 100:14 by weight and has a 65-minute gel time at 25 deg C, providing a longer application window than the 946 hardener version. It can be cured for five days at 25 deg C or heat-cured for two hours at 77 to 93 deg C after room-temperature gel. Handling and machining are typically possible after 16 to 24 hours at room temperature.

Key features

  • Extended working window: The mixed system has a 65-minute gel time at 25 deg C.
  • Solvent-free laminating system: The unfilled epoxy is used for composite manufacture, repair, and filament winding.
  • Room-temperature or heat cure: The system supports a five-day room-temperature cure or a two-hour elevated-temperature cure after gel.

Applications

  • Composite structure manufacture
  • Composite repair
  • Filament winding
Product Family

EPOCAST 50-A1/9816

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
White
Pot Life Pot Life
2-5 minutes
Physical Properties
Viscosity (Part A) Viscosity (Part A)
7,770 mPa.s
Viscosity (Part B) Viscosity (Part B)
250 mPa.s
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
68 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-received and handling values for the resin, hardener, and mixed system.

Property Value Unit Method / condition
Color 50-A1 resin amber; 9816 hardener straw; mixed system amber - Visual
Viscosity 50-A1 7,770; 9816 250; mixed 2,400 cP At 25 deg C
Mix ratio by weight 100:14 - 50-A1 resin:Hardener 9816
Gel time 65 min At 25 deg C
Shelf life 12 months Components unopened under the stated storage conditions
System type Unfilled, solvent-free - Two-component epoxy laminating system
Technical properties

After-processing / final-state properties

Cure and handling characteristics define the final cured-state preparation.

Property Value Unit Method / condition
Room-temperature cure 5 days At 25 deg C
Elevated-temperature cure 2 h At 77 to 93 deg C after room-temperature gel
Handling and machining 16 to 24 h At room temperature
Flammability Self-extinguishing - Cured laminating system