Huntsman Epocast 50A1/9816
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Two-Component Epoxy System
- 7,770 mPa s Resin Viscosity
- EPOCAST 50-A1/Hardener 9816 System
Product Description
EPOCAST® 50-A1 Resin with Hardener 9816 is a two-component epoxy material system comprising EPOCAST® 50-A1 epoxy resin and Hardener 9816. The resin is supplied as an epoxy constituent with a reported dynamic viscosity of 7,770 mPa·s at 20°C and density of 1.2 g/cm³ at 25°C. Hardener 9816 is a lower-viscosity curing component with a reported dynamic viscosity of 250 mPa·s and density of 1.02 g/cm³ at 25°C. The supplied resources do not establish the mix ratio, working life, cure schedule, supported substrates, applications, or cured performance of the combined system.
Key features
- Two-component epoxy system: Combines EPOCAST® 50-A1 epoxy resin with Hardener 9816 as separate resin and curing components.
- Resin viscosity: EPOCAST® 50-A1 has a reported dynamic viscosity of 7,770 mPa·s at 20°C.
- Low-viscosity hardener: Hardener 9816 has a reported dynamic viscosity of 250 mPa·s at 25°C.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Reported physical properties of the individual EPOCAST® 50-A1 resin and Hardener 9816 components. These SDS values are not presented as product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Component function | Epoxy constituent / hardener | — | EPOCAST® 50-A1 resin / Hardener 9816 |
| Dynamic viscosity | 7,770 / 250 | mPa·s | EPOCAST® 50-A1 at 20°C / Hardener 9816 at 25°C |
| Density | 1.2 / 1.02 | g/cm³ | EPOCAST® 50-A1 / Hardener 9816; 25°C |
| Relative density | 1.21 / 1.02 | — | EPOCAST® 50-A1 / Hardener 9816 |
| Water solubility | Partly soluble / practically insoluble | — | EPOCAST® 50-A1 / Hardener 9816; 20°C |