EPOXYLITE E8112 Hi Temp Epoxy Potting Compound is a two-component heat-cured potting compound supplied as a viscous liquid resin and powder hardener. It is used for bench casting, vacuum casting, and the potting or sealing of electrical and electronic components requiring high-temperature resistance. The system mixes at 100:50 by weight, with resin conditioning at 65 to 85 deg C to reduce viscosity and support bubble release. The mixed compound has an 8 to 12 hour pot life at room temperature and supports several elevated-temperature cure schedules.

Key features

  • Bench and vacuum casting: The compound is documented for both conventional bench casting and vacuum casting.
  • Eight-to-twelve-hour pot life: The mixed system provides an extended room-temperature application window.
  • Multiple heat-cure options: Four cure schedules allow time and temperature to be selected for the assembly process.

Applications

  • Bench casting
  • Vacuum casting
  • Potting and sealing high-temperature electrical and electronic components
Product Family

EPOXYLITE E8112

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Component, mixing, conditioning, and pot-life data before cure.

Property Value Unit Method / condition
Resin form Viscous liquid - As supplied
Hardener form Powder - As supplied
Mix ratio by weight 100:50 - Resin:hardener
Recommended resin conditioning 65 to 85 deg C Before adding the powder hardener
Pot life 8 to 12 h Mixed system at room temperature
Technical properties

After-processing / final-state properties

Cure options and bounded high-temperature performance statements.

Property Value Unit Method / condition
Cure options 16 h at 93 deg C; 4 h at 121 deg C; 1 h at 177 deg C; or 30 min at 204 deg C - Heat-cure schedules captured for the exact product
High-temperature property range At least 260 deg C Electrical and physical properties
Short-duration temperature exposure > 316 deg C Short-period exposure