FREKOTE AC4368
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- Combined Mold Release and Conditioning
- Multi-Resin Molding Compatibility
- 5 to 10-Minute Solvent Evaporation
Product Description
LOCTITE® FREKOTE® AC4368 is a clear, one-part, silicone-based mold release agent containing a lubricant for release and mold-surface conditioning. The liquid can be brushed or sprayed onto clean metal or plastic mold surfaces, where the solvent evaporates to leave a thin release film. It is suitable for molding processes using epoxy, polyurethane, and polyester materials with room-temperature or elevated-temperature cure systems.
Key features
- Multipurpose release: Supports release applications involving epoxy, polyurethane, and polyester molding materials.
- Surface conditioning: Contains a lubricant that conditions the mold surface while forming the release film.
- Flexible application: Can be applied by brushing or spraying and used with room-temperature or elevated-temperature cure systems.
Applications / Suitable for
- Release and conditioning of metal and plastic molds
- Epoxy, polyurethane, and polyester molding systems
- Room-temperature and elevated-temperature cure processes
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical as-supplied characteristics and storage information for LOCTITE® FREKOTE® AC4368.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Physical form | Liquid | — | As supplied |
| Appearance | Clear | — | Visual |
| Odor | Hydrocarbon | — | As supplied |
| Solvent | Hexane | — | Solvent carrier |
| Specific gravity | 0.72 | — | Typical product value |
| Shelf life | 18 | months | From date of manufacture |