FREKOTE B-15
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- One-Part Polymeric Mold Sealing
- 30-Minute Recoat Window
- 24-Hour Full-Cure Sealing
Product Description
LOCTITE® FREKOTE® B-15 is a clear, colorless, one-part, solvent-based polymeric mold sealer formulated for preparing composite and metal molds with micro-porosity, minor surface scratches, or other small imperfections. It forms a base coat that seals the mold surface before application of a compatible FREKOTE® mold release agent. The sealer provides high thermal stability and is formulated to avoid contaminating transfer to molded parts, supporting consistent mold preparation and release-system performance.
Key features
- Mold-surface sealing: Seals micro-porosity, minor scratches, and small surface imperfections.
- Composite and metal mold compatibility: Formulated for preparing both composite and metal mold surfaces.
- Base-coat function: Used with compatible FREKOTE® products to support the mold release system.
- Non-contaminating transfer: Formulated to avoid transfer of contaminating material to molded parts.
- High thermal stability: Supports mold preparation for elevated-temperature molding processes.
Applications / Suitable for
- Preparation and sealing of composite molds
- Preparation and sealing of metal molds
- Molds with micro-porosity, minor scratches, or small surface imperfections
- Base-coat preparation before application of compatible FREKOTE® mold release products
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Documented as-supplied characteristics and application timing for LOCTITE® FREKOTE® B-15.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Liquid mold sealer | — | One-part polymeric system |
| Appearance | Clear, colorless | — | As supplied |
| Carrier type | Solvent based | — | As supplied |
| Drying time between coats | 30 | min | At 20°C |
| Full cure time | 24 | h | At 20°C |
After-processing / final-state properties
Documented characteristics of the cured mold-sealing base coat.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Surface finish | Matte | — | Cured sealer finish |
| Transfer behavior | No contaminating transfer | — | Documented product characteristic |
| Thermal characteristic | High thermal stability | — | No numerical temperature limit stated on the supplied product page |