Product Description
LOCTITE® FREKOTE® R-120 is a one-part, water-based, semi-permanent release agent for rubber molding. Applied as a finely atomized spray to a preheated mold, it chemically bonds to the surface and forms a thin, inert, thermally stable release coating. The product supports natural and synthetic rubber polymers, including some thermoplastic urethanes, across mold application temperatures from 60°C to 200°C. It is intended for demanding molding processes where minimal mold buildup and low transfer to the molded part are required.
Key features
- Water-based formulation: Supplied as a translucent, non-flammable emulsion with mild odor.
- Semi-permanent release coating: Chemically bonds to a preheated mold surface to support multiple releases.
- Broad application-temperature range: Suitable for mold temperatures from 60°C to 200°C.
- Fast heat cure: Full cure time decreases as mold temperature increases, reaching 4 minutes at 150°C.
- Controlled mold condition: Recommended where minimal mold buildup and low transfer to molded parts are required.
Applications / Suitable for
- Natural and synthetic rubber molding
- Some thermoplastic urethane molding applications
- Demanding molding processes requiring minimal mold buildup
- Preheated molds operating from 60°C to 200°C
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Documented as-supplied characteristics and application conditions for LOCTITE® FREKOTE® R-120.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Translucent emulsion | — | As supplied; LMS-controlled characteristic |
| Chemical type | Water-based emulsion | — | One-part semi-permanent release agent |
| Odor | Mild | — | As supplied |
| Specific gravity | 0.98–1.02 | — | At 25°C |
| pH | 3.9–4.1 | — | LMS-controlled characteristic |
| Application temperature | 60–200 | °C | Preheated mold surface |
| Full cure time | 25 / 10 / 4 | min | At 60°C / 93°C / 150°C, respectively |
| Optimal storage temperature | 8–21 | °C | Unopened container in a dry location |
After-processing / final-state properties
Documented characteristics of the heat-cured LOCTITE® FREKOTE® R-120 release coating.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Cured thermal stability | ≤315 | °C | Heat-cured release coating |
| Release-film form | Thin, inert coating | — | Chemically bonded to a properly prepared, preheated mold surface |
| Epoxy release test | ≥4 | — | LMS-controlled cured-material test |
| Finish reflection | Matte | — | Henkel product-page technical specification |