HARDENER HY 5049

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

HARDENER HY 5049

Main features

  • High-Strength Structural Bonding
  • Documented Water/Ice/Tropical-Climate Resistance
  • Transparent Cured Bondline

Product Description

ARALDITE® 5049 A/B is a two-part epoxy laminating adhesive that cures to a transparent bondline, making it highly suitable for fabricating composite parts such as snow skis and snowboards. This system requires a heat cure for optimal results and is engineered to bond effectively to a wide variety of materials commonly used in the ski industry.

Key features

  • High structural integrity: Formulated to deliver high strength under both static and dynamic loading conditions.
  • Environmental durability: Provides robust resistance to challenging outdoor conditions, including water, ice, and tropical climates.
  • Aesthetic finish: Creates a transparent bondline that preserves the visual quality of laminated recreational equipment.

Applications / Suitable for

  • Laminating snow skis and snowboards.
  • Fabricating composite archery limbs.
  • Bonding honeycomb core facing.
Product Family

HARDENER HY 5049

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio Mix Ratio
100:54
Pot Life Pot Life
75 (Gel time) minutes
Mechanical Properties
Elongation Elongation
6% %

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure physical and processing characteristics of ARALDITE® 5049 A/B.

Property Value Unit Method / condition
Appearance / Color (Mixed) Amber Liquid - Visual
Mix Ratio (Volume) 100:54 - Part A to Part B
Mix Ratio (Weight) 100:43 - Part A to Part B
Viscosity (Mixed System) 2800 cP at 25°C, ASTM D2393
Density (Mixed System) 1.08 g/cm³ ASTM D792
Gel Time 75 minutes at 25°C, 100 g
Technical properties

After-processing / final-state properties

Cured mechanical and thermal properties of ARALDITE® 5049 A/B.

Property Value Unit Method / condition
Hardness 86 Shore D ASTM D2240
Ultimate Tensile Strength 10,000 (69) psi (MPa) ASTM D638
Elongation 6 % ASTM D638
Tensile Modulus 400,000 (2758) psi (MPa) ASTM D638
Glass Transition Temperature (Tg) 223 (106) °F (°C) DMA, Cured 15 min @ 212°F (100°C), ASTM D4065