HumiSeal 1B31EPA Acrylic Conformal Coating
Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others
Main features
- Fast drying
- MIL‑I‑46058C qualified
- IPC‑CC‑830 compliant
Product Description
HumiSeal 1B31EPA is a fast‑drying, single‑component acrylic conformal coating designed to provide excellent moisture and environmental protection for printed circuit assemblies. The cured film exhibits outstanding flexibility, fluoresces under UV light for easy inspection, and allows straightforward repair. HumiSeal 1B31EPA is MIL‑I‑46058C qualified, IPC‑CC‑830 compliant, RoHS Directive 2002/95/EC compliant, and EPA 33/50 compliant.
Product Key Features
- Single‑component acrylic formulation
- Fast drying, enabling efficient throughput
- MIL‑I‑46058C qualified
- IPC‑CC‑830 compliant
- RoHS compliant (Directive 2002/95/EC)
- EPA 33/50 compliant
Applications
- Protection of printed circuit boards (PCBs) across industrial, automotive, aerospace, and consumer electronics
Packaging
Please select Package Size.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Density (g)
Density (g)
0.95 g/cm3
Film Thickness
Film Thickness
25 - 75 µm
Solids
Solids
28 %
Physical Properties
Viscosity
Viscosity
325 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
Glass Transition Temperature (Tg)
14 °C
Operating Temperature
Operating Temperature
-65 - 125 °C
Electrical Properties
Breakdown Voltage
Breakdown Voltage
6300 V