HumiSeal Thinner 505

Harmonization Code : 3814001000 |

HumiSeal Thinner 505

Main features

  • RoHS Directive 2015/863/EU compliant
  • Ensures proper viscosity adjustment
  • Compatible with HumiSeal 1R32 and 1R32A-2

Product Description

HumiSeal Thinners are blends of solvents, formulated to maintain the original system balance when added to the correct coating type. These HumiSeal® Thinners are in full compliance with the RoHS  Directive 2015/863/EU. 

Product Key Features

  • Ensures proper viscosity adjustment for HumiSeal conformal coatings
  • Fully compliant with  RoHS Directive 2015/863/EU. 

Applications

  • Adjusting viscosity of HumiSeal 1R32 and 1R32A-2 conformal coatings.
Product Family

HUMISEAL 505

1. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity Specific Gravity
0.83
Vapor Density Vapor Density
3.5
Vapor Pressure Vapor Pressure
0.0203927 kg/cm2
Thermal Properties
Boiling Point Boiling Point
117 °C
Flash Point Flash Point
14 °C

Additional Information

Directions for Use   

Add HumiSeal® Thinner to a compatible coating until the desired viscosity is obtained.  

Handling Precautions  

HumiSeal® Thinners are flammable and the following standard safety precautions should be observed:  

  • Use only in well ventilated areas.   
  • Protective gloves and goggles should be worn.   
  • In case of prolonged skin contact, wash with water.   
  • In case of eye contact, flush with water and contact physician.   
  • Avoid prolonged breathing of vapors.  
  • Unused portions of HumiSeal® products must be disposed of in strict compliance with Local, State, and  Federal laws governing such matters.   
  • Consult the Safety Data Sheet (SDS) for more specific product information. 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers