INSULCAST 116 FR-FC

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

INSULCAST 116 FR-FC

Main features

  • Equal-Ratio Production-Line Epoxy Potting
  • 9,800 cP Mixed Viscosity
  • UL 94 V-0 Classification

Product Description

INSULCAST® 116 FR-FC Epoxy Potting Compound is a two-component, equal-ratio epoxy potting and casting compound designed for production-line mixing and automatic dispensing. The black Part A and cream Part B may be mixed 1:1 by weight or volume, producing a typical mixed viscosity of 9,800 cP and a 30 to 45-minute pot life. The system cures at room temperature or through an accelerated heat schedule and is recognized for UL 94 V-0 flammability. Typical cured properties include Shore D 75 hardness, 65.5 MPa tensile strength, 0.65 W/m·K thermal conductivity, and 420 V/mil dielectric strength.

Key features

  • Equal-ratio production system: The two components mix 1:1 by weight or volume for manual or automated dispensing.
  • 30 to 45-minute pot life: Typical mixed viscosity is 9,800 cP.
  • Flame-retardant cured epoxy: The system is recognized for UL 94 V-0 and has 0.65 W/m·K thermal conductivity.

Applications / Suitable for

  • Production-line electronic potting
  • Automatic dispensing and casting
  • Flame-retardant electrical insulation

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Part A color Black N/A As supplied
Part B color Cream N/A As supplied
Part A viscosity 7,200 cP ASTM D2393
Part B viscosity 11,000 cP ASTM D2393
Mix ratio 1:1 ratio By weight or volume
Mixed viscosity 9,800 cP Typical
Pot life 30 to 45 min 100 g mass
Cure options 16 to 24 h at 22°C; 2 h at 22°C plus 2 h at 55°C N/A Documented schedules
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 75 Shore D ASTM D2240
Compressive strength 79.3 MPa ASTM D695
Tensile strength 65.5 MPa ASTM D638
Flexural strength 69.0 MPa ASTM D790
Tensile elongation 5 to 7 % ASTM D638
Thermal conductivity 0.65 W/m·K Typical cured value
Dielectric strength 420 V/mil ASTM D149
Flammability classification V-0 UL 94 Documented recognition

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers