INSULCAST 140 FR

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

INSULCAST 140 FR

Main features

  • Epoxy Casting with Insulcure 11B
  • 50,000 cP Mixed Viscosity
  • 2.3 W/(m K) Thermal Encapsulation

Product Description

INSULCAST® 140 FR with INSULCURE® 11B is a black, two-component epoxy casting and encapsulation system formulated for high thermal conductivity and Class F operating properties. The resin is combined with INSULCURE 11B at a published ratio of 100:3 to 4 by weight and has a typical mixed viscosity of 50,000 cP. The system is documented for electrical insulation and heat transfer in demanding electronic assemblies. Typical cured properties include Shore D 90 to 95 hardness, 2.3 W/m·K thermal conductivity, 420 V/mil dielectric strength, and service from -55°C to 155°C.

Key features

  • High thermal conductivity: Typical cured thermal conductivity is 2.3 W/m·K.
  • Class F operating properties: The system is documented for elevated-temperature electrical encapsulation.
  • Rigid electrical insulation: Typical cured data include Shore D 90 to 95 hardness and 420 V/mil dielectric strength.

Applications / Suitable for

  • Thermally conductive electrical casting
  • Electronic potting and encapsulation
  • Assemblies requiring Class F operating properties
Product Family

INSULCAST 140 FR

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color Black N/A Mixed system
Mix ratio 100:3 to 4 parts by weight INSULCAST 140 FR : INSULCURE 11B
Mixed viscosity 50,000 cP Typical
Pot life 150 min At 25°C
Reference cure 2 h At 120°C
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 90 to 95 Shore D Typical cured value
Thermal conductivity 2.3 W/m·K Typical cured value
Dielectric constant 6.3 N/A At 1 kHz
Dielectric strength 420 V/mil Typical cured value
Volume resistivity 1 × 10¹⁵ ohm·cm Typical cured value
Coefficient of thermal expansion 26 × 10⁻⁶ 1/°C Typical cured value
Service temperature -55 to 155 °C Documented range
Flammability classification V-1 UL 94 Published portfolio classification